Mn13 Nm500 Ar500 qotishma po'lat plitalar aşınmaya bardoshli po'lat plitalar
Xitoyning yetakchi yetkazib beruvchi va ishlab chiqaruvchisi sifatida GNEE Steel nikel asosidagi qotishma mahsulotlarni-tejamkorlik bilan ta'minlaydi.
- E-xat yuboring:ss@gneesteel.com
- Tel:+8615824687445
Mn13 Nm500 Ar500 qotishma po'lat plitalar aşınmaya bardoshli po'lat plitalar
Mahsulot tavsifi
NM400 NM500 aşınmaya bardoshli po'lat plitalar aşınma plitalari
Ishqalanishga chidamli plastinka AR400 AR500
Aşınmaya bardoshli po'lat
Qattiq po'lat plitalar
qattiq 500 qattiq 400
po'lat plitalarni kesish va bükme
Mahsulot tavsifi
1.Ishlab chiqarish jarayoni
1)Steelmakjarayonning oqim diagrammasi
Blast furance+Issiq metall ladler+KRIssiq metallga ishlov berish+konvertor+LF tozalash pechi+RH vakuumli gazsizlantirish pechi+kon-quyma
2. Rolling jarayonining oqim sxemasi
Qayta isitiladigan pech+Yuqori bosimli suvli kireqni tozalash+qirrali tegirmon+qo‘pol ishlov berish tegirmoni+pardozlash tegirmoni+Tezlashtirilgan sovutish+Issiq tekislash moslamasi+Markalash va purkagichli bosib chiqarish+sovutish to‘shagi+Onlayn UT+O‘simliklarni kesish+Ikki tomonlama qirqish+kesish uchun uzunlik Kesish+O‘lchash+Markalash va Spray Chop etish+Sovuq tekislash/Issiqlik bilan ishlov berish
3.Issiqlik bilan ishlov berish sxemasi
Plitalar+Shotli portlatish+Söndürme pechi+Söndürme mashinasi+Temperlash pechi+Issiq tekislagich+sovutuvchi yotoq+kesish+Sovuq tekislagich+Bezatish va qadoqlash
4. Qalinligi va kengligi
Qalinligi: 4,5mm-150mm
Kengligi: 1600mm-4100mm
5.Asosiy sinf
Germaniya: XAR400, XAR450, XAR500, XAR600, Dillidur400, Dillidur500
Belgiya: QUARD400, QUARD450, QUARD500
Frantsiya: FORA400, FORA500, Creusabro4800, Creusabro8000
Baosteel: B-HARD360, B-HARD400, B-HARD450, B-HARD500
HBIS: NM360, NM400, NM450, NM500
Finlyandiya: RAEX400, RAEX450, RAEX500
Yaponiya: JFE-EH360, JFE-EH400, JFE-EH500, WEL-HARD400, WEL-HARD500
6.Kimyoviy tarkibi va xossasi
| Baho | c | Si | Mn | P | S | Al | Cr+Ni+Mo | Nb+V+Ti |
| NM400 | 0.10-0.40 | 0.20-0.40 | 1.00-2.00 | Maks 0.015 | Maks 0.003 | Minimal 0.020 | Maks 0.9 | Izlanish miqdori |
| NM450 | 0.10-0.40 | 0.20-0.40 | 1.00-2.00 | Maks 0.015 | Maks 0.003 | Minimal 0.020 | Maksimal 1.2 | |
| NM500 | 0.10-0.40 | 0.20-0.45 | 1.00-2.00 | Maks 0.015 | Maks 0.003 | Minimal 0.020 | Maksimal 1,5 | |
| NM550 | 0.10-0.50 | 0.20-0.45 | 1.00-1.50 | Maks 0.015 | Maks 0.003 | Minimal 0.020 | Maksimal 2.0 | |
| NM600 | 0.10-0.50 | 0.20-0.45 | 1.00-1.50 | Maks 0.015 | Maks 0.003 | Minimal 0.020 | Maksimal 2,5 | |
| XCHD400 | 0.10-0.30 | 0.20-0.40 | 1.00-2.00 | Maks 0.015 | Maks 0.003 | Minimal 0.020 | Maks 0.1 | |
| XCHD450 | 0.10-0.40 | 0.20-0.40 | 1.00-2.00 | Maks 0.015 | Maks 0.003 | Minimal 0.020 | Maks 0.9 | |
| XCHD500 | 0.10-0.40 | 0.20-0.45 | 1.00-2.00 | Maks 0.015 | Maks 0.003 | Minimal 0.020 | Maksimal 1,5 |
7.
| Baho | Hajmi (mm) | RP0.2(Mpa) | Rm(Mpa) | A50(%) | AKV,(ºC) | KV2(J) | HBW | ||
| NM400 | 100 | 1233 | 1337 | 15 | -20 | 35 | 37 | 42 | 415 |
| NM450 | 60 | 1345 | 1434 | 9.5 | -20 | 72 | 59 | 58 | 455 |
| NM500 | 50 | 1608 | 1706 | 10.5 | -20 | 43 | 50 | 45 | 495 |
| XCHD400 | 35 | 1025 | 1161 | 17.5 | -40 | 52 | 45 | 40 | 413 |
| XCHD450 | 30 | 1281 | 1400 | 10.5 | -40 | 45 | 48 | 52 | 453 |
| XCH500 | 6 | 1465 | 1529 | 13.5 | -40 | 24 | 24 | 22 | 515 |
8. Sertifikatlar
9 Tasniflash jamiyati
ISO 9001 sertifikati
9. Qadoqlash va jo'natish
Konteyner yoki quyma yuk kemasi bilan dengizga qadoqlash
Yetkazib berish muddati: 7 kun ichida stok hajmi; 40 kun ichida yangi material
10. Bizning xizmatlarimiz
Biz po'lat plitalarni mijozning talabiga binoan yoki chizmasiga ko'ra kesishimiz va egishimiz mumkin, mijozlar talabiga binoan qadoqlashimiz mumkin.
11. Ilova
Kam uglerodli, past oltingugurtli, past fosforli va mikro qotishmalarning kombinatsiyalangan kimyoviy tarkibi dizaynini qabul qilib, oflayn söndürme va boshqa ilg'or avtomatlashtirish texnologiyalarini qo'llash orqali bizning aşınmaya bardoshli (Aşınmaya chidamli) plastinka uyda va chet elda mashhur. Asosan issiqlik elektr stantsiyasi, ko'mir konlari, tsement tegirmonlari, yuklash mashinalari, tog'-kon mashinalari, loyiha mashinalari uchun ishlatiladi. Metallurgiya mashinalari, aşınmaya bardoshli plastinka qum tegirmoni silindrsimon qobiq, qanot, hovlida va portda ishlatiladigan mexanik qismlarda, rulman tuzilishida ham qo'llanilishi mumkin. Ehtiyot qismlar va boshqalar.
Issiq teglar: mn13 nm500 ar500 qotishma po'lat plitalar aşınmaya bardoshli po'lat plitalar, Xitoy mn13 nm500 ar500 qotishma po'lat plitalar aşınmaya bardoshli po'lat plitalar etkazib beruvchilar
Sizga ham yoqishi mumkin
So'rov yuborish