Incoloy 800 po'lat plitalar
Xitoyning yetakchi yetkazib beruvchi va ishlab chiqaruvchisi sifatida GNEE Steel nikel asosidagi qotishma mahsulotlarni-tejamkorlik bilan ta'minlaydi.
- E-xat yuboring:ss@gneesteel.com
- Tel:+8615824687445
Gnee Super Alloy (Tianjin) Co., Ltd. Xitoyda incoloy 800 po'lat plitasining eng professional ishlab chiqaruvchilari va yetkazib beruvchilaridan biridir. Agar siz Xitoyda ishlab chiqarilgan yuqori sifatli incoloy 800 po'lat plitalarini butunlay sotmoqchi bo'lsangiz, fabrikamizdan bepul namuna olishga xush kelibsiz. Yaxshi xizmat va o'rtacha narx mavjud.
800 qotishmasi quyidagi xususiyatlarga ega: Bu yuqori quvvatli nikel-temir-xrom qotishmasi boʻlib, u yuqori haroratlarda kuchli oksidlanish va karbonizatsiyaga chidamliligi hamda suv bilan koʻp muhitlarda korroziyaga chidamliligiga ega.
800 :800 metallografik struktura yuz-markazlangan kubik panjarali strukturadir. Juda past uglerod miqdori va yaxshilangan Ti: C nisbati strukturaning barqarorligini va sensibilizatsiya va donalararo korroziyaga maksimal qarshilikni oshiradi. Taxminan 950 daraja past haroratli tavlanish nozik kristall tuzilishini ta'minlaydi.

Mahsulot nomi Nikel qotishmasi C276 C22 C4 B2 B3 Hastelloy X plastinka varag'i
Materiallar Monel / Inconel / Hastelloy / Dupleks po'lat / PH po'lat / Nikel qotishmasi
Shakl dumaloq, zarb, halqa, lasan, gardish, disk, folga, sferik, lenta, kvadrat, bar, quvur, varaq
Dupleks darajasi: 2205 (UNS S31803/S32205), 2507 (UNS S32750), UNS S32760 (Nol 100), 2304,904L
Boshqalar: 253Ma,254SMo,654SMo,F50(UNS S32100)F60,F61,F65,1J22,N4,N6 va boshqalar
Qotishma: Qotishma 20/28/31;
Hastelloy: Hastelloy B/ -2/B-3/C22/C-4/S/ C276/C-2000/G-35/G-30/X/N/g;
Hastelloy B / UNS N10001, Hastelloy B-2 / UNS N10665 /
DIN W. Nr . 2.4617, Hastelloy C, Hastelloy C-4 / UNS N06455 / DIN W. Nr . 2.4610, Hastelloy C-22 / UNS N06022 / DIN W. Nr . 2.4602, Hastelloy C-276 /
UNS N10276 / DIN W. Nr . 2.4819, Hastelloy X / UNS N06002 / DIN V. Nr. 2.4665
Haynes: Haynes 230/556/188;
Inconel seriyasi:
Inconel 600/601/602CA/617/625/713/718/738/X-750, Duradgor 20;
Inconel 718 / UNS N07718 / DIN W. Nr. 2.4668, Inconel 601 / UNS N06601 / DIN W. Nr. 2.4851,
Inconel 625 / UNS N06625 / DIN W. Nr. 2.4856,Inconel 725 / UNS N07725,Inconel X-750 / UNS N07750 / DIN W. Nr. 2.4669,Inconel 600 / UNS N06600 /{{13}r.
Incoloy: Incoloy 800/800H/800HT/825/925/926;
GH: GH2132, GH3030, GH3039, GH3128, GH4180, GH3044
Monel: Monel 400/K500/R405
Nitronic: Nitronic 40/50/60;
Nimonic: Nimonic 75/80A/90/A263;

1-savol: Namuna miqdorini buyurtma qila olamanmi?
A1: Ha, bizda MOQ yo'q.
2-savol: O'z logotipimni qutilarga/kartonlarga qo'shishim mumkinmi?
A2: Ha, OEM va ODM bizdan mavjud.
3-savol: Distribyutor bo'lishning afzalliklari nimada?
A3: Maxsus chegirmali marketing himoyasi.
Issiq teglar: incoloy 800 po'lat plitalar, Xitoy incoloy 800 po'lat plitalar yetkazib beruvchilar