Nikel qotishma Monel 400 oyna plitasi
Quvur: ph6-273mm; d1-30 mm; uzunligi 1000-8000 mm
Bar: ph4-200mm; uzunligi 2000-6000 mm
Chiziq: 0,05 * 5,0-5,0 * 250 mm
Tel: 0,01-10 mm
Xitoyning yetakchi yetkazib beruvchi va ishlab chiqaruvchisi sifatida GNEE Steel nikel asosidagi qotishma mahsulotlarni-tejamkorlik bilan ta'minlaydi.
- E-xat yuboring:ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. Xitoyda nikel qotishma monel 400 oyna plitasining eng professional ishlab chiqaruvchilari va yetkazib beruvchilaridan biridir. Agar siz Xitoyda ishlab chiqarilgan yuqori sifatli nikel qotishma monel 400 oyna plitasini butunlay sotmoqchi bo'lsangiz, fabrikamizdan bepul namuna olishga xush kelibsiz. Yaxshi xizmat va o'rtacha narx mavjud.
Qotishma Monel 400 oyna plitasi taqdimoti
Nikel qotishma Monel 400 plastinka


Monel 400 Plitalar dilerlari, Monel 400 Sheets, Monel Alloy 400 Cilalı Plitalar, Monel 400 Shims Stock, Xitoy Monel 400 Plitalar Narxlari, AMS 4544 Monel Alloy 400 tavlangan chiziqlar, Xitoy Monel 400 Sovuq haddelenmiş plastinka dilerlari, Monel Supplies00.
Monel 400 - nikel va misning ikkilik qotishmasi (oz miqdorda temir, marganets, uglerod va kremniy). Qotishma yuqori quvvatga ega, kislotali va gidroksidi muhitga yuqori qarshilik va yaxshi süneklik va issiqlik o'tkazuvchanligiga ega. Monel 400 noldan 1000 daraja F (538 daraja) gacha bo'lgan haroratlar uchun javob beradi. U faqat sovuq ishlov berish orqali qattiqlashishi mumkin.
Monel 400 plitalari spetsifikatsiyasi:
| Texnik xususiyatlari | : | ASTM B127 |
| O'lchamlari | : | ASTM, ASME |
| Hajmi | : | 1000 mm x 2000 mm, 1220 mm x 2440 mm, 4' x 8', 1250 mm x 2500 mm, 1500 mm x 3000 mm dan 6000 mm gacha, 2000 mm x 4000 mm dan 6000 mm gacha |
| Tugatish | : | Issiq haddelenmiş plastinka (HR) 2B, 2D, BA NO(8), SATIN (Plastik qoplamali) |
| Shakl | : | Bobinlar, plyonkalar, rulolar, oddiy varaq, chiziq, yassi, bo'sh (doira), halqa (gardish) va boshqalar. |
| Turi | : | ASTM B 127 Monel 400 plitalari |
Nikel qotishmasi 400 plastinka, varaq va tasmaning texnik xususiyatlari
| Hajmi | Varaq | Plita | Ip |
|---|---|---|---|
| Qalinligi | <6 mm | 6 mm dan katta yoki unga teng | 0,15 mm - 3 mm |
| Kengligi | 1200 mm dan kam yoki unga teng | 2800 mm dan kam yoki unga teng | 1000 mm dan kam yoki unga teng |
| Uzunlik | 3000 mm dan kam yoki unga teng | 8000 mm dan kam yoki unga teng | Mijozning talabi sifatida |
Nikel qotishmasining kimyoviy tarkibi 400 (%)
| Element | Ni (nikel) | Cu (mis) | Fe (temir) | C (uglerod) | Mn (marganets) | Si (kremniy) | S (oltingugurt) |
|---|---|---|---|---|---|---|---|
| Min | 63 | 28 | – | – | – | – | – |
| Maks | – | 34 | 2.5 | 0.3 | 2 | 0.5 | 0.024 |
GNEE kompaniyasining muhiti
Nikel 400 oynali plastinka

GNEE Group zavod muhiti
Nikel qotishmasi 400 oyna plitasi

TSS
1-savol: Xarid qilishdan oldin qanday mahsulot haqida ma'lumot berishim kerak?
Iltimos, daraja, kenglik, qalinlik va sirtni qayta ishlash talablarini, shuningdek sizga kerak bo'lgan miqdorlarni taqdim eting.
2-savol: Qanday yuk tashish portlari mavjud?
Biz odatda Shanxay, Tyanjin, Qingdao va Ningbo portlaridan jo'natamiz.
3-savol: Sizning to'lov shartlari qanday?
30% T/T oldindan va 70% balans jo'natishdan oldin yoki BL nusxasi yoki ko'rishda LC asosida.
Issiq teglar: Nikel qotishma Monel 400 oyna plitasi, Xitoy nikel qotishma Monel 400 oyna plitasi yetkazib beruvchilari
Sizga ham yoqishi mumkin
So'rov yuborish