Zanglamaydigan po'latdan 329 430 Plitalar
Uglerod (C): 0,12% dan kam yoki unga teng
Kremniy (Si): 0.75% dan kam yoki unga teng
Marganets (Mn): 1 dan kam yoki unga teng.00%
Fosfor (P): 0.040% dan kam yoki unga teng
Oltingugurt (S): 0 dan kam yoki unga teng.030%
Nikel (Ni): 0.60% dan kam yoki unga teng (qoʻshilishi mumkin)
Chromium (Cr):16.00~18.00%
kimyoviy tarkibi
Uglerod (C): 0,12% dan kam yoki unga teng
Kremniy (Si): 0.75% dan kam yoki unga teng
Marganets (Mn): 1 dan kam yoki unga teng.00%
Fosfor (P): 0.040% dan kam yoki unga teng
Oltingugurt (S): 0 dan kam yoki unga teng.030%
Nikel (Ni): 0.60% dan kam yoki unga teng (qoʻshilishi mumkin)
Chromium (Cr):16.00~18.00%
Mexanik xususiyatlar
Zichlik: 7,75 g/sm³
Erish nuqtasi: 1427 daraja
Kengayish koeffitsienti: mm/daraja (20-100 daraja)
Young moduli: kN/mm²
Qattiqlik moduli: kN/mm²
Ilova standarti: yoʻq (UNS)

Issiq teglar: zanglamaydigan po'latdan 329 430 plastinka, Xitoy zanglamaydigan po'latdan 329 430 plastinka yetkazib beruvchilar