ASTM A36 issiq haddelenmiş yumshoq po'latdan yasalgan katak plastinka ASTM A36 / A36M A283 GRC
video

ASTM A36 issiq haddelenmiş yumshoq po'latdan yasalgan katak plastinka ASTM A36 / A36M A283 GRC

ASTM A36 Issiq haddelenmiş yumshoq po'latdan yasalgan katak plitasi ASTM A36 / A36M A283 GRCDescriptionWidth: 600-2500mm Darajasi: Q235B A36Ilova: Payvandlash uglerodli po'lat materiallari Texnikasi: Issiq haddelenmiş Turi: Chelik Plitalar Standarti: {ASTMLength mm} Qora Qalinligi: 0.5-100mm Material: Q235Mahsulot nomi: Plitalar Shakli: Yassi po'lat PlitalarCoil Og'irligi: 3-8 Tonna Og'irligi: Reuglar SpangleYuqori yorug'lik: past karbonli po'lat plitalar karbonli po'lat plitalar
So'rov yuborish
Hozir chat

Xitoyning yetakchi yetkazib beruvchi va ishlab chiqaruvchisi sifatida GNEE Steel nikel asosidagi qotishma mahsulotlarni-tejamkorlik bilan ta'minlaydi.

Mahsulotni tanishtirish

 

ASTM A36 issiq haddelenmiş yumshoq po'latdan yasalgan katak plastinka ASTM A36 / A36M A283 GRC

Tavsif

Kengligi: 600-2500mm Darajasi: Q235B A36
Ilova: Karbonli po'latdan yasalgan materiallarni payvandlash Texnika: Issiq haddelenmiş
Turi: Chelik plastinka Standart: ASTM
Uzunlik: 1000-12000mm Yuzaki ishlov berish: Qora
Qalinligi: 0.5-100mm Material: Q235
Mahsulot nomi: Plita Shakl: Yassi po'lat plitalar
Bobinning og'irligi: 3-8 tonna Shiqillagan: Oddiy spangle
Yuqori yorug'lik:

past karbonli po'lat plitalar

,

karbonli po'lat plitalar

A36 varaqlar va plitalarning texnik xususiyatlari

A36 varaqlari va plitalari uchun texnik xususiyatlar. Agar bu yerda biron bir spetsifikatsiya ko'rsatilmagan bo'lsa, tez taklif qilish uchun kontakt tugmasidan foydalaning.

Texnik xususiyatlari ASTM A36 / ASME SA36
Standart AISI, ASTM, BS, DIN, GB, JIS
Qalinligi 0.5-100mm
Ixtisoslash Shim varaq, teshilgan varaq, BQ profili.
Uzunlik 2000-12000 mm
Shakl Bobinlar, plyonkalar, rulolar, oddiy varaq, shim varag'i, teshilgan varaq, katakli plastinka, tasma, yassi, bo'sh (doira), halqa (gardish)
Tugatish Issiq haddelenmiş plastinka (HR), Sovuq haddelenmiş varaq (CR), 2B, 2D, BA NO(8), SATIN (Plastik qoplamali)
Qattiqlik Yumshoq, qattiq, yarim qattiq, chorak qattiq, bahor qattiq va boshqalar.
Baho MS A36, (UNS K02600)

A36 varaqlar va plitalar Kimyoviy tarkibi

 

Baho min maks
C 0.25 0.290
Cu 0.20
Fe 98.0
Mn 1.03
P 0.040
Si 0.280
S 0.050

 

A36 varaqlari va plitalarining mexanik xususiyatlari

Xususiyatlari Metrik Imperator
Zichlik 7,85 g/sm3 0,284 funt/dyuym3
Kuchlanish kuchi, yakuniy 400 - 550 MPa 58000 - 79800 psi
Chidamlilik, hosildorlik 250 MPa 36300 psi
Uzilishdagi cho'zilish (200 mm da) 20.0 % 20.0 %
Sinishi cho'zilishi (50 mm da) 23.0 % 23.0 %
Elastiklik moduli 200 GPa 29000 ksi
Ommaviy modul (po'lat uchun odatiy) 140 GPa 20300 ksi
Puasson nisbati 0.260 0.260
Kesish moduli 79,3 GPa 11500 ksi

 

A36 varaqlar va plitalar – ekvivalent baholar

STANDART MS A36
WERKSTOFF NR. 50049 3.1
UNS K02600

 

 

 

A36 rulonlari

A36 UNS K02600 bobinlari

A36 WERKSTOFF NR. 50049 3.1 Bobinlar

A36 chiziqlar

A36 UNS K02600 chiziqlar

A36 WERKSTOFF NR. 50049 3.1 Chiziqlar

 

 

A36 plyonkalari

A36 UNS K02600 plyonkalari

A36 WERKSTOFF NR. 50049 3.1 folga

A36 Shim varaq

A36 UNS K02600 Shim varaq

A36 WERKSTOFF NR. 50049 3.1 Shim varaq

ASTM A36 Hot Rolled Mild Steel Checkered Plate  ASTM A36 / A36M A283 GRC 0ASTM A36 Hot Rolled Mild Steel Checkered Plate  ASTM A36 / A36M A283 GRC 1ASTM A36 Hot Rolled Mild Steel Checkered Plate  ASTM A36 / A36M A283 GRC 2

Issiq teglar: astm a36 issiq haddelenmiş yumshoq po'latdan yasalgan katakli plastinka astm a36 / a36m a283 grc, Xitoy astm a36 issiq haddelenmiş yumshoq po'latdan yasalgan katak plastinka astm a36 / a36m a283 grc etkazib beruvchilari

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov