Monel 400 2. Yuvilgan trubka 4360 qotishma
video

Monel 400 2. Yuvilgan trubka 4360 qotishma

N04400-ni yo'q qilishning yumshatilgan naycha xususiyatlari

Yaxshi veldorlik
Yuqori kuch
Egiluvchanlik
Shakllanish
So'rov yuborish
Hozir chat

Xitoyning yetakchi yetkazib beruvchi va ishlab chiqaruvchisi sifatida GNEE Steel nikel asosidagi qotishma mahsulotlarni-tejamkorlik bilan ta'minlaydi.

Mahsulotni tanishtirish

400 2. 4360 shuvli trubka bilan tanishing

Monel 400 2. 4360 yumaloq quvur

monel 400 2.4360 Alloy round Pipemonel 400 2.4360 Alloy round Pipe

Nikel 400 yeneallangan truba, shuningdek, Superoloy deb nomlanuvchi, 926 darajali tahsil olish mumkin. Monel 400 chirishsiz naycha ma'lum bir kislotalarga qarshi tura oladi, ayniqsa yuqori haroratlarda gidroblor va sulfat kislotalarga tegishli bo'lgan ba'zi dasturlar uchun mos emas. Kislotali sharoitlardan farqli o'laroq, alloy 400 chalsiz naycha nafaqat ishqorli echimlarga, balki tuzli suv va dengiz suviga, shuningdek, dengizga tegishli dasturlarga mos keladigan ajoyib qarshilik ko'rsatadi.

Monel 400 quvur o'lchamlari

ANSI / ASME B36.19 ga binoan 400 ta oqilona quvurlar beriladi.
Wt=Monel 400 quvur devorining qalinligi
OD=Monel 400 trubkadan tashqarida

ASTM B165 Monel 400 quvur
mm
Quvur
mm
ichida. Sch Kg / m
13.72 1.65 1/4 10S 0.50
13.72 2.24 1/4 40S 0.64
13.72 3.02 1/4 80S 0.81
17.15 1.65 3/8 10S 0.64
17.15 2.31 3/8 40S 0.86
17.15 3.20 3/8 80S 1.12
21.34 2.11 1/2 10S 1.02
21.34 2.77 1/2 40S 1.29
21.34 3.73 1/2 80S 1.65
26.67 2.11 3/4 10S 1.30
26.67 2.87 3/4 40S 1.71
26.67 3.91 3/4 80S 2.23
33.40 2.77 1 10S 2.13
33.40 3.38 1 40S 2.54
33.40 4.55 1 80S 3.29
33.40 6.352) 1 160 4.30
42.16 2.77 10S 2.73
42.16 3.56 40S 3.44
42.16 4.85 80S 4.53
42.16 6.352) 160 5.69
48.26 2.77 10S 3.16
48.26 3.68 40S 4.11
48.26 5.08 80S 5.49
60.33 2.77 2 10S 3.99
60.33 3.91 2 40S 5.52
60.33 5.54 2 80S 7.60
60.33 8.742) 2 160 11.29
73.03 3.05 10S 5.35
73.03 5.16 40S 8.77
73.03 7.01 80S 11.59
88.90 3.05 3 10S 6.56
88.90 5.49 3 40S 11.47
88.90 7.62 3 80S 15.51
88.90 11.132) 3 160 21.67
101.60 3.05 10S 7.53
101.60 5.74 40S 13.78
101.60 8.08 80S 18.92
114.30 3.05 4 10S 8.50
114.30 6.02 4 40S 16.32
114.30 8.56 4 80S 22.67
114.30 13.492) 4 160 34.05
141.30 6.55 5 40S 22.10
141.30 9.53 5 80S 31.44
141.30 15.882) 5 160 49.87
168.28 3.4 6 10S 14.04
168.28 7.11 6 40S 28.69
168.28 10.97 6 80S 43.21
168.28 14.27 6 120 54.75
168.28 18.262) 6 160 68.59
219.08 8.18 8 40S 43.20
219.08 12.7 8 80S 65.63
219.08 18.23 8 120 91.30
219.08 23.012) 8 160 112.97

Monel 400 N04400 quvurini kimyoviy formulasi

Baho C Mn Si S Ku Fok Ni
Monel 400 0. 30 max 2. 00 max 0. 50 Max 0. 024 max 28.00 – 34.00 2.50 max 63. 00 min

Gne Group fabrikasi Atrof-muhit

Monel 400 2. 4360 yilni yumshatdi

monel 400 2.4360 Alloy round annealed Pipe


GNEE GROUP Mahsulotni qadoqlash

400 2. 4360 qotishuv quvuri quvur

monel 400 2.4360 Alloy round annealed Pipe

TSS

Savol: Sizning kompaniyangizning afzalliklari qanday?
Javob: Bizda boshqa zamonaviy temir kompaniyalarga qaraganda ko'proq mutaxassislar, texnik xodimlar, ko'proq raqobatbardosh narxlar va sotishdan keyingi xizmat ko'rsatamiz.
Savol: Qancha mamlakatlarga eksport qildingiz?
Javob: 50 dan ortiq mamlakatlarga asosan AQSh, Rossiya, Buyuk Britaniya, Quvayt, Misr, Turkiya, Iordaniya, Hindiston va boshqa mamlakatlarga eksport qilinadi.
Savol: Siz namunalarni taqdim qila olasizmi?
Javob: Ha. Biz bilan bog'lansangiz, biz bepul kichik namunalarni zaxirada berishimiz mumkin. Mosisionlashtirilgan namunalar kunlar 5-7 ni oladi.

Issiq teglar: Monel 400 2

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov