Tayyorlangan 2205 zanglamaydigan po'latdan yasalgan kvadrat quvur
Model NO.201, 202 SertifikatlashRoHS, ASTM, GB, JISShapeFlatTechniqueIssiq haddelenmiş Yuzaki ishlov berishCilalanganO'lchamlar Sizning talablaringiz bo'yicha
So'rov yuborish
Hozir chat
Xitoyning yetakchi yetkazib beruvchi va ishlab chiqaruvchisi sifatida GNEE Steel nikel asosidagi qotishma mahsulotlarni-tejamkorlik bilan ta'minlaydi.
- E-xat yuboring:ss@gneesteel.com
- Tel:+8615824687445
Mahsulotni tanishtirish
Tayyorlangan 2205 zanglamaydigan po'latdan yasalgan kvadrat quvur
| Zanglamaydigan po'latdan yasalgan to'rtburchaklar quvur uchun mavjud o'lcham | |||||||
| Kvadrat quvur | |||||||
| Diametri | Diametri | Diametri | Diametri | Diametri | Diametri | Diametri | Diametri |
| 10x10 mm | 12x12 mm | 15x15 mm | 16x16 mm | 17x17 mm | 18x18 mm | 19x19 mm | 20x20 mm |
| 21x21 mm | 22x22 mm | 24x24 mm | 25x25 mm | 25,4x25,4 mm | 28x28 mm | 28,6x28,6 mm | 30x30 mm |
| 32x32 mm | 35x35 mm | 37x37 mm | 38x38 mm | 40x40 mm | 45x45 mm | 48x48 mm | 50x50 mm |
| 80x80 mm | 100x100 mm | ||||||
| Devor qalinligi:{0}}.25-4.0mm | |||||||
| To'rtburchak quvur | |||||||
| Diametri | Diametri | Diametri | Diametri | Diametri | Diametri | Diametri | Diametri |
| 6x10 mm | 8x16 mm | 8x18 mm | 9x19 mm | 10x20 mm | 10x22 mm | 11x21,5 mm | 11,6x17,8 mm |
| 12x14 mm | 12x34 mm | 12,3x25,4 mm | 13x23 mm | 14x20 mm | 14x24 mm | 14x72 mm | 15x30 mm |
| 15x35 mm | 15x88 mm | 16x26 mm | 17,5x15,5 mm | 18x35 mm | 17x37 mm | 19x38 mm | 20x30 mm |
| 20x40 mm | 22x25 mm | 22x26 mm | 25x38 mm | 25x30 mm | 25x40 mm | 25x50 mm | 27x40 mm |
| 30x40 mm | 30x50 mm | 30x60 mm | 30x70 mm | 40x60 mm | 45x75 mm | 40x80 mm | 50x100 mm |
| 42x114 mm | |||||||
| Devor qalinligi:{0}}.25-4.0mm | |||||||
| Kimyoviy tarkibi | |||||||
| Baho | C dan kichik yoki teng | Si dan kichik yoki teng | Mn dan kichik yoki teng | P dan kichik yoki teng | S dan kichik yoki teng | Ni | Cr |
| 201 | 0.15 | 1 | 5.50-7.50 | 0.5 | 0.03 | 3.50-5.50 | 16.00-18.00 |
| 202 | 0.15 | 1 | 7.50-10.00 | 0.5 | 0.03 | 4.00-6.00 | 17.00-19.00 |
| 304 | 0.08 | 1 | 2 | 0.045 | 0.03 | 8.00-11.00 | 18.00-20.00 |
| 304L | 0.03 | 1 | 2 | 0.045 | 0.03 | 8.00-12.00 | 18.00-20.00 |
| 309 | 0.2 | 1 | 2 | 0.04 | 0.03 | 12.00-15.00 | 22.00-24.00 |
| 309S | 0.08 | 1 | 2 | 0.045 | 0.03 | 12.00-15.00 | 22.00-24.00 |
| 310 | 0.25 | 1 | 2 | 0.04 | 0.03 | 19.00-22.00 | 24.00-26.00 |
| 310S | 0.08 | 1 | 2 | 0.045 | 0.03 | 19.00-22.00 | 24.00-26.00 |
| 316 | 0.08 | 1 | 2 | 0.045 | 0.03 | 10.00-14.00 | 16.00-18.00 |
| 316L | 0.03 | 1 | 2 | 0.045 | 0.03 | 10.00-14.00 | 16.00-18.00 |
| 316Ti | 0.08 | 1 | 2 | 0.045 | 0.03 | 10.00-14.00 | 16.00-18.00 |
| 410 | 0.15 | 1 | 1 | 0.04 | 0.03 | 0.6 | 11.50-13.50 |
| 430 | 0.12 | 0.12 | 1 | 0.04 | 0.03 | 0.6 | 16.00-18.00 |
Issiq teglar: moslashtirilgan 2205 zanglamaydigan po'latdan yasalgan kvadrat quvur, Xitoy moslashtirilgan 2205 zanglamaydigan po'latdan yasalgan kvadrat quvur etkazib beruvchilari