ASTM A312 TP316 / TP316L quvurlari tanishtirildi
ASTM A312 TP316 / TP316Ldan yasalgan choksiz quvurlar ishlab chiqarishning istalgan bosqichida payvandlashni o'z ichiga olmaydi; Payvandlash jarayoni paytida payvandlangan quvurlar payvandlash jarayoni paytida plitka metalini qo'shma ravishda ishlab chiqariladi. TP316 / TP316L quvuri issiqlik bilan davolanadi, unda quvurni isitiladi va barcha xrom karbidlari to'liq behisob yoki erigan bo'lishi mumkin. Keyingi suvni sovutish yoki tez sovutish, g'alla chegaralarida karbinlarning yog'ingarchiliklarini ta'minlash uchun olib boriladi. Bundan tashqari, TP316l tezkor xronlarni karbinlarni TP316 ga nisbatan pastroq deb biladi. Bu, ehtimol, cheklangan sezgiga, shuning uchun foydani payvandlash, olov kesish va boshqa issiq ishchi operatsiyalarga olib kelishi mumkin.
ASTM A240 tipidagi 316 naychasini standart spetsifikatsiya qilish
| Texnik xususiyatlari | ASTM A240 / ASME SA240 | ||||||
| Qalinlik | 0. 5m -100 mm | ||||||
| Tashqi diametr | 10 mm, 25,4 mm, 38,1,8, 50,8 mm, 250mm, 250mm, 300mm, 350mm, 350mm va boshqalar | ||||||
| Uzunligi | 2000 mm, 2440 mm, 3000mm, 5800 mm, 6000mm, 6000mm va boshqalar | ||||||
| Sirtmoq | 2b, 2D, BA, 2-chi, №4, 8k, 8k, Soch chiziq, qumli portlash, cho'tka, cho'tka, cho'tka va boshqalar | ||||||
| Tugatmoq | Issiq rulonli (HR), sovuq rulonli naycha (CR), 2b, 2D, BA yo'q (8), atlas (plastik qoplangan) | ||||||
| Shakl | Dumaloq naycha to'rtburchaklar naycha va hokazo. | ||||||
316 Ro'y yokiture tarkibi va mexanik xususiyatlari
| Baho | C | Mn | Si | P | S | Kri | Mor | Ni | N | |
| 316L | Min. Maks. |
/ 0.03 |
/ 2.0 |
/ 1.0 |
/ 0.045 |
/ 0.030 |
16.00 18.00 |
2.0 3.0 | 12.00 15.00 |
/ |
| 316 | Min. Maks. |
/ 0.03 |
/ 2.0 |
/ 1.0 |
/ 0.045 |
/ 0.030 |
16.00 17.00 |
2.0 3.0 | 11.00 14.00 |
/ |
| 317 | Min. Maks. |
/ 0.08 |
/ 2.0 |
/ 1.0 |
/ 0.035 |
/ 0.030 |
18.00 10.00 |
3.0 4.0 | 11.00 15.00 |
/ |
O'lchamlari, o'lchamlari va taligi
| Nps | *t/D | Bardoshlik,% nominaldan | |
|---|---|---|---|
| 1/8"~2.5" | Hamma | +20.0 | -12.5 |
| 3"~18" | 5% dan kam yoki unga teng | +22.5 | -12.5 |
| 3"~18" | >5% | +15.0 | -12.5 |
| Katta yoki 20 ga teng " Wld. |
Hamma | +17.5 | -12.5 |
| Katta yoki 20 ga teng " smls |
5% dan kam yoki unga teng | +22.5 | -12.5 |
| Katta yoki 20 ga teng " smls |
>5% | +15.0 | -12.5 |
| Baho | Mustahkamlik chegarasi (MPA) |
Kuch berish kuchi 0. 2% isboti (MPA) |
Cho'zish (% 50 mm) |
Qattiqlik | |
| Rockwell b (Hr b) |
Pinel (Hb) |
||||
| 316 | 515 | 205 | 40 | 92 | 201 |
| 316L | 515 | 205 | 40 | 90 | 187 |
| 317 | 520 | 205 | 35 | 90 | 187 |
* T: Nominal devor qalinligi; D: tashqi diametrli buyurtma qilingan.



AsTM A312 TP316 / TP316L tarbiyasiz quvurlar odatda 1/2 "24 dan", ASTM A312 TP316 / TP316L tp316 "48" dan peldasi mavjud. Devor qalinligi Asme b36.1 0} m yoki asMe b36,9 m9 metrga muvofiq jihozlanadi. Quvurlar odatda 6,096 m (20 '), 12.19 va 12 m, va hokazolarda, belgilangan uzunlikdan oshadi va tavsiya etilgan uzunlikdagi [6 mm] dan oshmaydi.
316 zanglamaydigan po'lat naychaning ekvivalent materiallari
| Baho | Yo'q. | Eski inglizlar | EURARMMM | China GB | Yapon jis | ||
| Bs | Ro'mol | Yo'q | Ism | ||||
| 316L | S31600 | 316ls15 | 58E | 1.4408 | X5CRNI 18-10 | 0 cr17ni14 | Sys316l |
| 316 | S31603 | 316S12 | – | 1.4401 | X2cnin 18-9 | 0 CR18ni9 | Sys316 |
GNEE GROUP Mahsulotni qadoqlash

TSS
Savol: Sizning fabrikangizga tashrif buyurishimiz mumkinmi?
Javob: Sizning jadvalingiz mavjud bo'lgandan so'ng, samimiy xush kelibsiz.
Savol: Sizda sifat nazorati bormi?
Javob: Ha, biz BV, SGS autentifikatsiyasini qo'lga kiritdik.
Savol: Siz jo'natishni tashkil qila olasizmi?
A: Shubhasiz, bizda eng ko'p kema kompaniyasidan eng yaxshi narxga ega bo'lishi va professional xizmat ko'rsatishni taklif qiladigan doimiy ekspeditor o'tkazuvchimiz bor.