Ta'riflar Karbonli po'lat A333 GR6 Strukturaviy quvur A234, A333 GR6, A106Suyuq trubkasi 20# q295b-e, q345b-eYuqori bosimli qozon trubkasi 20G 15MnG 20MnG 15G2SMor, sa 06c, sa210a, sa210c, A333P2, A333P11, A33P12, A333P22, A33P36, A333P91, A333P92, A335T2, A335T11, A335T12, A335T22, A335T91, A335T23, A335T9Pipeline API SPEC 5L, X6, X6, X4, X65, , ASTM A106, ASTM A333, BS301, BS3602, BS3603, BS3604 , PSL1, PSL2, DNV-OS-F101, CSA-Z245 Qotishma quvur 4140, 42CrMo, 32CrMo, 15CrMo,
So'rov yuborish
Hozir chat

Xitoyning yetakchi yetkazib beruvchi va ishlab chiqaruvchisi sifatida GNEE Steel nikel asosidagi qotishma mahsulotlarni-tejamkorlik bilan ta'minlaydi.

Mahsulotni tanishtirish

 

ASME B16.9 Karbonli po'latdan burmalar A234 WPB / A333 GR6 / A106 GRB-BG kriogen trubkasi

Tavsif

Sertifikatlash: Idoralar, ISO, BV, SGS Mahsulot nomi: Karbonli po'lat A333 GR6 kriogenli quvur
OD: 12mm-620mm Devor qalinligi: 0.25mm-45mm
Uzunlik: 1000mm-12000mm Shakl: Dumaloq
Standart: ASTM, AISI, JIS, DIN, EN, GB Texnika: ERW
Namuna: Ruxsat berilgan Ilova: Mashinasozlik
Yuqori yorug'lik:

karbonli po'latdan choksiz quvur

,

og'ir po'lat quvur

ASME B16.9 burmalari, karbonli po'lat A234 WPB / A333 GR6 / A106 GRB--BG kriogen naycha

 

Tavsiflar Karbonli po'lat A333 GR6 kriogenli quvur
Strukturaviy quvur

A234, A333 GR6, A106

Suyuq quvur 20# q295b-e, q345b-e
Yuqori bosimli qozon trubkasi

20G 15MnG 20MnG 15CrMoG, 12Cr1MoVG

St35.8, sa106b, sa106c, sa210a, sa210c, A333P2, A333P11, A33P12, A333P22, A33P36, A333P91, A333P92, A335T2, A335T51T, A335T11T, A335T11, 335T23, A335T9

Quvur liniyasi

API SPEC 5L, X42, X52, X60, X65,X70,X80

ASTMA53, ASTM A106, ASTM A333, BS301, BS3602, BS3603, BS3604, PSL1, PSL2, DNV-OS-F101, CSA-Z245

Qotishma quvur 4140, 42CrMo, 32CrMo, 15CrMo,
Qadoqlash Qora bo'yoq, lak bilan bo'yash, brezentli qadoqlash
Oxiri Umumiy dumaloq uchi, qiyshiq.
Qayta ishlash galvanizatsiya; kesish; quvurdan tashqarida ip yasash; Ishlov berish.

 

Ishlab chiqarish tavsifi

1) Aniq quvur tasvirlari, foydalanish va standart

ASME B16.9 Bends Carbon Steel A234 WPB / A333 GR6 / A106 GRB-BG Cryogenic Tube 0

 

ASME B16.9 Bends Carbon Steel A234 WPB / A333 GR6 / A106 GRB-BG Cryogenic Tube 1

 

ASME B16.9 Bends Carbon Steel A234 WPB / A333 GR6 / A106 GRB-BG Cryogenic Tube 2

 

Foydalanish:Shlangi quvur, suyuqlik trubkasi, jismoniy konstruktsiya, gidravlik qurilma, avtomobil qismlari, po'lat gilza, podshipnik, gidravlik silindr, pnevmatik silindr va gidravlik quvur

 

Standart:ISO, JIS, GB, DIN, ASTM, API

 

2) Kimyoviy tarkibi

 

Tez-tez ishlatiladigan toifadagi nozik quvurning kimyoviy tarkibi

Standart Baho Kimyoviy tarkibi (%)
    C Si Mn S P Cr
GB/T699 10# 0.07~0.13 0.17~0.37 0.35~0.65 0 dan kichik yoki unga teng.035 0 dan kichik yoki unga teng.035  
GB/T3639-2000 20# 0.17~0.23 0.17~0.37 0.35~0.65 0 dan kichik yoki unga teng.035 0 dan kichik yoki unga teng.035  
GB3077-88 35# 0.32~0.39 0.17~0.37 0.35~0.65 0 dan kichik yoki unga teng.035 0 dan kichik yoki unga teng.035  
  45# 0.42~0.50 0.17~0.37 0.50~0.80 0 dan kichik yoki unga teng.035 0 dan kichik yoki unga teng.035  
  40kr 0.37~0.44 0.17~0.37 0.50~0.80 0 dan kichik yoki unga teng.035 0 dan kichik yoki unga teng.035 0.08~1.10
  25Mn 0.22~0.29 0.17~0.37 0.70~1.00 0 dan kichik yoki unga teng.035 0 dan kichik yoki unga teng.035 0 dan kichik yoki unga teng.25
  37Mn5 0.30~0.39 0.15~0.30 1.20~1.50 0 dan kichik yoki unga teng.015 0.020 dan kichik yoki unga teng  

 

3) Mexanik xossalari

 

Umumiy nozik quvurning mexanik xususiyatlari

Standart Baho Belgilanish (%)
    Sovuq tugagan (qattiq) (BK) Sovuq tugagan (Yumshoq) BKW
    UTS (yakuniy tortishish kuchi) singandan keyin foiz cho'zilishi UTS (yakuniy tortishish kuchi) singandan keyin foiz cho'zilishi
   
    s b (Mpa) δ 5(%) s b (Mpa) δ 5(%)
GB/T3639-2000 10# 410 dan katta yoki unga teng 6 dan katta yoki teng 375 dan katta yoki teng 10 dan katta yoki teng
GB3077-88 20# 510 dan katta yoki unga teng 5 dan katta yoki teng 450 dan katta yoki unga teng 8 dan katta yoki teng
  35# 590 dan katta yoki unga teng 4 dan katta yoki teng 550 dan katta yoki teng 6 dan katta yoki teng
  45# 645 dan katta yoki unga teng 4 dan katta yoki teng 630 dan katta yoki unga teng 5 dan katta yoki teng
  40kr 784 dan katta yoki unga teng 12 dan katta yoki teng    
  37Mn5 784 dan katta yoki unga teng 12 dan katta yoki teng    

 

Izohlar:

 

Sovuq tugagan (qattiq):Quvurlar oxirgi sovuq shakllanishdan keyin issiqlik bilan ishlov berilmaydi va shuning uchun deformatsiyaga nisbatan ancha yuqori qarshilikka ega

 

Sovuq tugagan (yumshoq):Yakuniy issiqlik bilan ishlov berishdan so'ng cheklangan deformatsiyani o'z ichiga olgan sovuq chizish amalga oshiriladi. Tegishli keyingi ishlov berish ma'lum darajada sovuq shakllanish imkonini beradi (masalan, egilish, kengayish)

 

Ilova maydoni:

Mexanik ishlov berish, mashinasozlik, avtomobilsozlik

 

4) Sifat nazorati

A. Ilg'or ishlab chiqarish uskunalari

B. Ishlab chiqarish oqimi

C. To'liq malakali va malakali ishchilar, ishlashdan oldin o'qitish va sinovdan o'tkazish

D. Sifatni qat'iy nazorat qilish tizimi

 

5) Qadoqlash va jo'natish

A) qadoqlash usuli

To'plamlarda kichik o'lchamlar, katta hajmdagi katta hajmli, ikkala uchini himoya qilish uchun plastik qopqoq bilan, dengizga mos qadoqlash yoki mijozning talabiga binoan.

 

B) Yuk tashish usuli

Mijozning talabiga binoan.

Odatda dengiz, havo, poezd yoki daryo va dengiz muvofiqlashtirilgan transportida.

 

TSS

Savol: To'lov muddati haqida nima deyish mumkin?

Javob: Odatda T / T yoki L / C, 30% depozit va yetkazib berishdan oldin 70%.

Savol: standart yetkazib berish sanasi haqida nima deyish mumkin?

Javob: Depozitni olgandan keyin 30 kun

Savol: Sizning imkoniyatlaringiz haqida nima deyish mumkin?

Javob: Po'lat quvurlar uchun oyiga 50,000 tonna, yiliga 600,000 tonna. Quvur armaturalari uchun yiliga 30,000 tonna

Savol: Sizning paketingiz haqida nima deyish mumkin?

Javob: Odatda mijozning talabiga binoan.

Umumiy qadoqlash ma'lumotlari: to'plamlarda kichik o'lchamlar, katta hajmdagi katta o'lchamlar, ikkala uchini himoya qilish uchun plastik qopqoqli ba'zi o'lchamlar, dengizga yaroqli qadoqlash.

Savol: Sizning asosiy bozoringiz va asosiy mijozlaringiz nima?

Javob: Biz po'lat quvurlar va quvur qismlari bo'yicha 12 yillik tajribaga egamiz. Bizning asosiy bozorimiz Xitoy, Singapur va boshqalarni o'z ichiga oladi. Asosiy mijozlar, jumladan HYST, Keppel guruhi va boshqalar.

Savol: Agar mahsulotlarda sifat muammosi bo'lsa, siz qanday munosabatda bo'lar edingiz?

Javob: Biz barcha sifat muammolarimiz uchun javobgar bo'lamiz.

Savol: Sizdan aniq narx/kotirovkani qanday olish mumkin?

Javob: Iltimos, bizga quyidagi tafsilotlarni ayting va biz sizga eng qisqa vaqt ichida taklifimizni yuboramiz:

1) Quvurning tashqi diametri

2) devor qalinligi

3) Bo'lim shakli (dumaloq, kvadrat va boshqalar)

4) Har bir quvur uchun uzunlik

5) Chelik darajasi

6) Standart (masalan: API 5L)

7) Buyurtma miqdori

8) Belgilanish (BK, BKW va boshqalar)

9) Savdo shartlari

PS: siz aniqlagan batafsil ma'lumot, biz aniqroq narxni taqdim etdik.

Issiq teglar: asme b16.9 egilgan karbonli po'latdan a234 wpb / a333 gr6 / a106 grb-bg kriogenli quvur, Xitoy asme b16.9 uglerodli po'latdan a234 wpb / a333 gr6 / a106 grb-bg kriogenli quvur yetkazib beruvchilar

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov