Model NO.8452Material zanglamaydigan po'latYuza ishlov berishCillatlanganFoydalanishMashinasozlik sanoatiBo'lim ShapeKvadratStandartAPI5l. API5c, ASTM A500, ASTM A554
So'rov yuborish
Hozir chat

Xitoyning yetakchi yetkazib beruvchi va ishlab chiqaruvchisi sifatida GNEE Steel nikel asosidagi qotishma mahsulotlarni-tejamkorlik bilan ta'minlaydi.

Mahsulotni tanishtirish

 

304, 201, 316, 316L payvandlangan A554 kvadrat quvur

 

Mahsulot: 304, 201, 316, 316L payvandlangan zanglamaydigan kvadrat quvur(Xitoy)

Biz haqimizda
Bizda ilg'or boshqaruv texnologiyasi bor, biz yaxshi sifatimiz tufayli ishonchni qozonamiz.
Bizda vijdonli va ishtiyoqli sotuvchimiz bor, biz mijozlarni eng yaxshi xizmatimiz bilan xursand qilamiz va barqaror qilamiz.
Biz chin yurakdan va sizning kompaniyamizga bo'lgan mehribon e'tiboringizni kutamiz.

mahsulot nomi 304, 201, 316, 316L payvandlangan zanglamaydigan kvadrat quvur (Xitoy)
hajmi OD (20*20mm-500*500mm)*VT(2mm-20mm)*L(6m-11,8m)
material 304, 201, 316L
standart API5L. API5C, ASTM A500
sirt Qora yo'qolgan, galvanizli, zangga qarshi moy va boshqalar.
foydalanuvchi Qurilish, suv isitish, avtomobil ishlab chiqarish, elektr o'rnatish va qazib olish va boshqalar.

Kimyoviy tarkibi:

Baho C dan kichik yoki teng Si dan kichik yoki teng Mn dan kichik yoki teng P dan kichik yoki teng S dan kichik yoki teng Ni Kamroq yoki teng Cr dan kichik yoki teng
201 0.12 0.75 7 0.045 0.045 1.00-1.28 13.70-15.70
202 0.15 1 2.25 0.045 0.045 4.07-4.17 14.00-16.00
304 0.08 0.75 2 0.045 0.03 8.00-11.00 18.00-20.00
304L 0.035 0.75 2 0.045 0.03 8.00-13.00 18.00-20.00
309 0.15 0.75 2 0.045 0.03 12.00-15.00 22.00-24.00
310S 0.08 1.5 2 0.045 0.03 19.00-22.00 24.00-26.00
316 0.08 1 2 0.045 0.03 10.00-14.00 16.00-18.00
316L 0.035 0.75 2 0.045 0.03 10.00-15.00 16.00-18.00
321 0.04-0.10 0.75 2 0.045 0.03 9.00-13.00 17.00-20.00
405 0.08 0.75 1 0.045 0.03 0.06 11.5-13.5
409 0.089 1 1 0.045 0.05 0.06 10.50-11.75
410 0.15 0.75 1 0.045 0.03 0.06 11.5-13.5
420 0.16-0.25 1 1 0.04 0.03 0.06 12.00-14.00
430 0.12 0.75 1 0.045 0.03 0.06 16.00-18.00
904L 0.02 1 2 0.045 0.03 23.00-28.00 19.00-23.00