Nickel270/N02270 Yuqori toza nikel qotishmasi

Nickel270/N02270 yuqori toza nikel qotishmasi

 

 

Nikel 270

Nikel 270 UNS N02270

Ip, lasan, folga va sim, ASTM F3

Nickel270 ilovasi

Qarshilik termometrlari, simli simlar, passiv katodlar, lyuminestsent lampalar komponentlari, elektrolitik hujayra anodlari

Nickel270 Tavsif

Qotishma 270 odatda kukunli metallurgiyadan tayyorlangan yuqori toza nikeldir. U past asosli qattiqlik va yuqori egiluvchanlikka ega. U asosan metall bo'lmagan qo'shimchalardan xoli.

Nickel270/N02270 high purity nickel alloy

Nickel270/N02270 high purity nickel alloy

Nikel270 Kimyosi tipik

Nikel + Kobalt: 99,9 dan katta yoki teng

Mis: 0 dan kichik yoki unga teng.01

Temir: 0 dan kichik yoki unga teng.05

Marganets: 0.003 dan kichik yoki unga teng

Uglerod: 0 dan kichik yoki unga teng.02

Oltingugurt: 0.003 dan kichik yoki unga teng

Titan: .005 dan kam yoki unga teng

Magniy: 0.005 dan kam yoki unga teng

Kremniy: 0.005 dan kichik yoki unga teng

Nikel270 jismoniy xususiyatlari

Zichlik: 0,322 lb/in3, 8,91 g/sm3

Qarshilik: ohm-cir-mil/ft, (μohm·m): 45.0 (0.075)

Maxsus issiqlik: BTU/lb- F daraja (J/g- K daraja): 0.110 (460)

Issiqlik o'tkazuvchanligi: BTU-in/soat-ft2- daraja F (Vt/m·- daraja): 595 (86)

O'rtacha issiqlik kengayish koeffitsienti: mkn/in- F (mkm/m- daraja) 70 - 200 F daraja (20 - 95 daraja ): 7,4 (13,3)

Elastiklik moduli: KSI (MPa) 30 x 103 (207 x 103) kuchlanish

Magnit o'tkazuvchanligi: ferromagnit

Erish diapazoni: 2650 daraja F (1454 daraja)

Nikel 270 shakli

Bobinlar - varaq, tasma, folga

Tel - profillar, yumaloq, tekis, kvadrat

Xona haroratida Nikel270 ning mexanik xususiyatlari

Xususiyatlari: tavlanish tipik

Maksimal kuchlanish kuchi: 50 KSI min (345MPa min)

Oqim kuchi: 16 KSI min (110 MPa min)

Cho'zilish: 50% min

Qattiqlik: Rb 66 maks.: Oʻlchov 0.010 dyuymdan katta yoki unga teng

Nickel270 xususiyatlari: Söndürme

Nikel 270 turli holatlarga sovuq ishlov berilishi mumkin.

Nikel270 issiqlik bilan ishlov berish

Nikel 270 issiqlik bilan ishlov berish orqali qattiqlashmaydi.

 