ASTM B127 K500 Nikel asosidagi qotishma plastinka
Standartlar: ASTM / ASME B127 / SB127
Olchamlari: 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm
Qalinligi: 0,1 mm dan 12 mm gacha
Xitoyning yetakchi yetkazib beruvchi va ishlab chiqaruvchisi sifatida GNEE Steel nikel asosidagi qotishma mahsulotlarni-tejamkorlik bilan ta'minlaydi.
- E-xat yuboring:ss@gneesteel.com
- Tel:+8615824687445
Gnee Super Alloy (Tianjin) Co., Ltd. Xitoyda astm b127 k500 nikel asosidagi qotishma plitasining eng professional ishlab chiqaruvchilari va yetkazib beruvchilaridan biri hisoblanadi. Agar siz Xitoyda ishlab chiqarilgan yuqori sifatli astm b127 k500 nikel asosidagi qotishma plastinkani butunlay sotmoqchi bo'lsangiz, fabrikamizdan bepul namuna olishga xush kelibsiz. Yaxshi xizmat va o'rtacha narx mavjud.
ASTM B127 K500 qotishma plastinka taqdimoti
ASTM B127 K500 Nikel qotishma plastinka


Monel K-500 plitasi mis va nikelning optimal kombinatsiyasi bilan mashhur bo'lib, uning korroziyaga chidamliligini oshiradi. Mahsulot endi qo'shimcha funktsiyalar bilan mavjud. Bu afzalliklar titan va alyuminiy birikmasidan kelib chiqadi, asos sifatida mis va nikel. Uning yaxshilangan xususiyatlari uning qattiqligi va mustahkamligidadir, bu mis va nikeldan foydalanish tufayli yog'ingarchilik fazalariga ta'sir qiluvchi issiqlik bilan ishlov berish orqali erishiladi. Ushbu davolash odatda qarish yoki yoshning qattiqlashishi deb ataladi.
Bunga qo'shimcha ravishda, u stressli korroziya yorilishiga chidamli va har qanday muhitga mos keladi. Uning unumdorligi 400 navidan uch baravar ko'p. Uning kuchi 1200 daraja F da o'zgarishsiz qoladi. Lekin harorat 400 daraja F ga ko'tarilganda uning egiluvchanligi va pishiqligi pasayadi. Bundan tashqari, uning erish nuqtasi ham 2400-2460 daraja F orasida. -200 daraja F gacha past haroratlarda u magnit bo'lmaydi.
Monel K{2}}500 varaqlari haqida bilishingiz kerak bo'lgan narsa shundaki, u qayta ishlanganidan keyin ma'lum magnit xususiyatlarga ega bo'ladi. Isitish vaqtida u tanlab oksidlanishga uchraydi va nikelga- boy magnit plyonka qoldiradi. Keyinchalik, normal ishlov berish jarayonida u hatto magnit bo'lmagan xususiyatlarini tiklaydi. Bugungi kunda ushbu choyshablarni ishlab chiqaradigan ishlab chiqaruvchilar ushbu materialga juda ehtiyotkorlik bilan munosabatda bo'lishadi, chunki ular hech qanday xato qilishni xohlamaydilar, aks holda u o'z xususiyatlarini yo'qotadi.
ASTM B127 Monel qotishmasi K500 varaq plastinkasining kimyoviy tarkibi
| Element | Monel K500 |
| C | 0,25 maks |
| Mn | 1,5 maks |
| Si | 0,5 maks |
| S | 0,010 maksimal |
| Cu | 27 – 33 |
| Fe | 0.5 – 2 |
| Ni | 63.00 min |
Monel K500 plitasining spetsifikatsiyasi
| N05500 Nikel qotishma plitalari spetsifikatsiyasi | ASTM B127 UNS N05500, ASME SB127, MSRR, AMS, BS |
|---|---|
| UNS N05500 Plitalar o'lchamlari (mm) | 1000 x 2000, 1220 x 2440, 1500 x 3000, 2000 x 2000, 2000 x 4000 |
| Qotishma K500 plastinka qalinligi | 0,1 dan 100 mm gacha |
| ASME SB 127 N05500 Plitalar kengligi | 10-2500 mm |
| DIN 2.4375 Qotishma K500 Plitalar uzunligi | 2m, 2.44m, 3m yoki kerak bo'lganda |
| ASTM B127 UNS N05500 varaq AMS | AMS |
| Monel Alloy K500 Plitasini tugatish | HR, CR, 2B, 2D, BA, NO(8), SATIN |
| WNR 2.4375 varaqning qattiqligi | Yumshoq, qattiq, yarim qattiq, chorak qattiq, bahor qattiq va boshqalar. |
| Monel K500 plitasi shaklida |
Qoplangan, Shim, Bo'sh, Yassi, Rolling, sovuq{0}}prokat, Protektor, tavlangan, o'lchami tozalangan, Rulolar, issiq{1}}o'ralgan, qirqib olingan, varaq, Plitka, Doira, folga, Ip, shashka, Yassilar, Bobinlar, yumshoq-tavlangan, |
ASME SB 127 UNS N05500 varaqining og'irligi
| Qalinligi | Birlik maydoni uchun plastinka og'irligi | Zichlik |
|---|---|---|
| 3/16 dyuym | 0,06000 funt/in²42,184176 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 1/4 dyuym | 0,08 funt/in²56,245568 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 3/8 dyuym | 0,121 funt/in²85,0714216 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 1/2 dyuym | 0,161 funt/in²113,1942056 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 5/8 dyuym | 0,196 funt/in²137,8016416 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 3/4 dyuym | 0,235 funt/in²165,221356 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 7/8 dyuym | 0,274 funt/in²192,6410704 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 1 dyuym | 0,313 funt/in²220,0607848 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 1 1/4 dyuym | 0,391 funt/in²274,9002136 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 1 1/2 dyuym | 0,47 funt/in²330,442712 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 1 3/4 dyuym | 0,549 funt/in²385,9852104 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 2 dyum | 0,627 funt/in²440,8246392 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 2 1/4 dyuym | 0,705 funt/in²495,664068 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 2 1/2 dyuym | 0,784 funt/in²551,2065664 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 2 3/4 dyuym | 0,862 funt/in²606,0459952 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
| 3 dyuym | 0,941 funt/in²661,5884936 kg/m² | 0,315 funt/dyuym³8,72 g/sm³ |
GNEE Group zavod muhiti
ASTM B127 K500 qotishma plastinka

GNEE kompaniyasining muhiti
monel ASTM B127 K500 qotishma plastinka

TSS
1-savol: Xarid qilishdan oldin qanday mahsulot haqida ma'lumot berishim kerak?
Iltimos, daraja, kenglik, qalinlik va sirtni qayta ishlash talablarini, shuningdek sizga kerak bo'lgan miqdorlarni taqdim eting.
2-savol: Qanday yuk tashish portlari mavjud?
Biz odatda Shanxay, Tyanjin, Qingdao va Ningbo portlaridan jo'natamiz.
3-savol: Sizning to'lov shartlari qanday?
30% T/T oldindan va 70% balans jo'natishdan oldin yoki BL nusxasi yoki ko'rishda LC asosida.
Issiq teglar: ASTM B127 K500 nikel asosidagi qotishma plastinka, Xitoy ASTM B127 K500 nikel asosidagi qotishma plastinka etkazib beruvchilari
Sizga ham yoqishi mumkin
So'rov yuborish