GH4169 va GH3536 (Hastelloy X): Ishlashni taqqoslash

 
 
 
GH4169 va GH3536 (Hastelloy X): Ishlashni taqqoslash
GH4169 vs GH3536 Hastelloy X Performance Comparison
01.

GH4169 va GH3536 (Hastelloy X): Ishlashni taqqoslash

GH4169 and GH3536 (Hastelloy X) are both high-performance nickel-based superalloys commonly used in the aerospace field, but they have different applications: GH4169 is a precipitation-hardening alloy with excellent strength below 650°C (e.g., turbine disks), while GH3536 is a solid solution alloy with better oxidation resistance and ductility at higher temperatures (>800 daraja ) (masalan, yonish kameralari).

02.

GH4169 nimaga ekvivalent?

Inconel 718

GH4169 (Amerika brendi Inconel 718ga ekvivalent) mukammal mexanik xossalari tufayli aerokosmik sanoatida keng qo'llaniladigan yog'ingarchilik{2}}qattiqlashtiruvchi nikel-asosli superqotishmadir (Lu va boshq., 2014).

GH4169 Equivalent

1. GH4169 va GH3536 kimyoviy tarkibini solishtirish (og'ir%)

Element GH4169 (Inconel 718) GH3536 (Hastelloy X) Asosiy farq
Nikel (Ni) 50.0 – 55.0 Balans (~ 65 dan katta yoki teng) GH3536 yuqori Ni ga ega
Xrom (Cr) 17.0 – 21.0 20.5 – 23.0 GH3536 yuqori Cr
Temir (Fe) Balans (~18-20) 17.0 – 20.0 GH4169 biroz yuqori Fe
Molibden (Mo) 2.80 – 3.30 8.0 – 10.0 GH3536 oyiga ~ 3 baravar ko'p
Kobalt (Kobalt) 1,00 dan kam yoki unga teng 0.5 – 2.5 GH3536 tarkibida Co
Volfram (Vt) 0.2 – 1.0 GH3536 tarkibida W
Niobiy (Nb) 4.75 – 5.50 GH4169 noyob– ″ oldingi
Titan (Ti) 0.65 – 1.15 GH4169 noyob
Alyuminiy (Al) 0.20 – 0.80 GH4169 noyob
Uglerod (C) 0,08 dan kam yoki unga teng 0.05 – 0.15 GH3536 yuqori C
Marganets (Mn) 0,35 dan kam yoki unga teng 1,00 dan kam yoki unga teng GH3536 yuqori
Silikon (Si) 0,35 dan kam yoki unga teng 1,00 dan kam yoki unga teng GH3536 yuqori
Fosfor (P) 0,015 dan kam yoki unga teng 0,040 dan kam yoki unga teng
Oltingugurt (S) 0,015 dan kam yoki unga teng 0,030 dan kam yoki unga teng
Bor (B) 0.002 – 0.006 0,010 dan kam yoki unga teng

 

2. GH4169 va GH3536 ning mexanik va ekologik xususiyatlarini taqqoslash

Xususiyat GH4169 (qotishma 718) GH3536 (Hastelloy X) Sanoat qarori
Mustahkamlash usuli Yog'ingarchilikning qattiqlashishi ( ′′) Qattiq eritma (Mo, Vt) GH4169 ko'proq og'irlik qiladi.
Maksimal xizmat harorati (yuklash) 700 daraja (1292 daraja F) 850 daraja - 950 daraja Strukturaviy yuk uchun GH4169.
Oksidlanish chegarasi (statik) 980 daraja 1200 daraja (2200 daraja F) GH3536 olovda g'alaba qozonadi.
Termal charchoq umri O'rtacha Elita (yorilishga qarshi turadi) GH3536 termal velosiped uchun.
Ishlab chiqarish qobiliyati Qiyin (tez qattiqlashadi) Yuqori (a'lo payvand) GH3536 mehnat xarajatlarini kamaytiradi.
Nikel tarkibi (Ni) ~ 53% ~ 47% GH4169 yuqori Nb tarkibiga ega.

GH4169 qotishma PDF faylini hozir yuklab olish uchun bosing

GH4169 va GH3536 ning ishlash dasturlari
GH3536 Alloy
03

GH3536 qotishmasi

GH3536o'zgaruvchan ochiq olov muhitiga ta'sir qiladigan komponentlar uchun sanoat standartidir.

Yuqori siklik oksidlanish ko'rsatkichi:Uning tarkibida yuqori xrom va temir moddasi mahkam yopishgan himoya qatlamini hosil qiladi, u hatto tez sovutish davrlarida ham tozalanmaydi.

Yuqori ishlov berish samaradorligi: GH3536oʻzining mukammal payvandlanishi bilan mashhur boʻlib,-murakkab yupqa devorli-yonish kamerasi va yondirgich qoplamalarini yorilishsiz yigʻish imkonini beradi.

Narx-Samarali yechim:Statik yong'in zonasi komponentlari uchun,GH3536eng yaxshi materialning ishlash muddati -samaradorligini taklif qiladi.

04

GH4169 qotishmasi

GH4169komponentlar haddan tashqari bosim ostida o'z shakllarini saqlab turishi kerak bo'lgan ilovalar uchun mos bo'lgan "Kuchli yuklarning qiroli".

Yuqori hosildorlik:ning hosildorligini saqlaydi1030 MPa dan katta yoki unga tengxona haroratida. Bu aylanadigan halqalar va turbinalar uchun tanlangan materialdir.

Yuqori tsiklli charchoq (HCF):Dvigatelning "sovuqroq" qismlarida (quyida) yuqori-chastotali mexanik tebranishlar natijasida yuzaga keladigan nosozliklarga qarshi turish uchun maxsus ishlab chiqilgan.700 daraja).

GH4169 Alloy
 
 

5. GH4169 va GH3536 ning umumiy ilovalari

GH4169 (Inconel 718):650 darajadan past haroratda ishlaydigan turbina disklari, mahkamlagichlar va yuqori{0}}kuchli issiq{1}}komponentlar .

GH3536 (Hastelloy X):Yonish kamerasining korpuslari, o'tish komponentlari va egzoz komponentlari.

Turbine disc
Turbinali disk
Fasteners
Mahkamlagichlar

Combustion chamber housing

Yonish kamerasining korpusi
Exhaust components
Egzoz komponentlari

 

Nikelga asoslangan qotishma yetkazib beruvchi-sifatida nega Gnee tanlaysiz?

✅️VIM + VAR erishi:GH4169 uchun majburiy ikki-vakuumli eritish uning charchoqqa chidamliligini maksimal darajada oshirib, nol ichki qo'shimchalarni ta'minlaydi.

✅️Aniq tekislik:Bizning aerokosmik varaqlarimiz sovutish teshiklarini avtomatlashtirilgan lazer bilan kesish uchun zarur bo'lgan ilg'or tekislashdan o'tadi.

✅️MTC 3.1 Kuzatilishi:Toʻliq EN 10204 3.1 Tegirmon sinovi sertifikatlari yuqori haroratning choʻzilishi va siqilish maʼlumotlarini tavsiflaydi.

✅️Ulgurji inventar:Biz ikkala sinfning katta zaxirasini saqlaymizChoksiz quvur, dumaloq chiziq va varaqshakllar tayyorTez global yetkazib berish.

Gnee Alloy GH4169(inconel 718) Certificate

Gnee Alloy GH4169 (inconel 718) sertifikati

 

📦 Qadoqlash va yetkazib berish

HammasiNikel asosidagi qotishmaMahsulotlar quyidagi usullar yordamida qadoqlanadi:

Yog'och palletlar yoki qutilar

Namlikka-o‘tkazmaydigan qadoq

Pech raqami, standart va o'lchamli teglar bilan etiketkalar

Dunyo bo'ylab dengiz, havo yoki ekspress orqali jo'natiladi

 Gnee Steel GH3030 Product Packing

Gnee Alloy GH4169 mahsulot qadoqlash

GH4169 Alloy uchun so'nggi eksport narxlari taklifi uchun biz bilan bog'laning

 

TSS

1-savol: GH4169 va GH3536 ni o'tish chizig'ida bir-biriga payvand qila olamanmi?
A: Ha.Ular mukammal metallurgiya muvofiqligiga ega. Turli termal kengayish zonalarida bo'g'inning barqaror bo'lishini ta'minlash uchun ERNiCr-3 yoki maxsus plomba metallaridan foydalanishni tavsiya etamiz.

 

2-savol: Nima uchun GH3536 yonish qoplamalari uchun 310S dan yaxshiroq?
Javob: 310S asosiy issiqlikka chidamli-po'lat bo'lsa-da,GH3536 nikel-asosidagi super qotishmamolibden bilan. U 310S ga qaraganda ancha yuqori siljish kuchi va termal charchoq yorilishiga nisbatan ancha yaxshi qarshilik ko'rsatadi.

 

3-savol: Qaysi qotishma qimmatroq?
Javob: Umuman olganda,GH4169 qimmatroqniobiy (Nb) miqdori yuqori boʻlgani va unumdorlik koʻrsatkichlariga erishish uchun murakkab koʻp bosqichli qarish issiqlik bilan ishlov berish (16+ soat) tufayli har kg uchun.

 

4-savol: Siz turbinali disklar va laynerlar uchun -oʻlchamlarga qarab{2}}kesilgan xizmatlarni taklif qilasizmi?
Javob: Albatta. taklif qilamizMaxsus ishlab chiqarishshtamplash yoki shakllantirish liniyasiga tayyor blankalarni yetkazib berish uchun, shu jumladan, nozik lazer va suv oqimi bilan kesish.