 1. Inconel625 (NO6625) qotishmasining umumiy ko'rinishi

Inconel 625 (NO6625) qotishmasiqattiq eritma mustahkamlangan va deformatsiyalangan yuqori-haroratli qotishma. U asosan oʻtga chidamli metallar niobiy va molibdenning qattiq eritmasi orqali nikel{2}}xrom matritsasini mustahkamlaydi. U juda ko'p ajoyib ishlash xususiyatlariga, yaxshi tashkiliy barqarorlikka ega va yuqori haroratli muhitda o'zining tarkibiy barqarorligini saqlab qolishi mumkin va uni o'zgartirish oson emas.

 

U mukammal korroziyaga chidamliligiga ega va oksidlovchi va kamaytiruvchi muhitda turli korroziy vositalarga mukammal qarshilikka ega. Azot kislotasi, fosforik kislota, sulfat kislota, xlorid kislotasi va ularning aralash kislotalari kabi noorganik kislotalar,Inconel 625 qotishmasimukammal korroziyaga chidamliligini ko'rsatishi mumkin. Bundan tashqari, xlorid muhitida qotishma chuqurchalar, yoriqlar korroziyasi, intergranulyar korroziya va eroziyaga mukammal qarshilik ko'rsatadi va xlorid ionini kamaytirish stressli korroziya yorilishiga samarali qarshilik ko'rsatishi mumkin. Hatto dengiz suvi va sanoat gaz muhitida yoki yuqori haroratlarda tuz eritmalari bilan aloqa qilishda ham korroziyaga olib kelishi qiyin.

 

Shu bilan birga, charchoq va o'rmalash xususiyatlariInconel 625 qotishmasiham nisbatan yaxshi, shuning uchun u takroriy kuchlar va uzoq muddatli stress ostida yaxshi ishlash holatini saqlab turishi mumkin-va charchoq yoriqlari, haddan tashqari deformatsiyalar va boshqa muammolarga moyil emas.

 

Ushbu ajoyib xususiyatlar bilan,Inconel 625 qotishmasiko'plab muhim sohalarda keng qo'llaniladi. Aerokosmik sohada u ko'pincha turbina qismlari, samolyot nozullari, yonish kamerasi komponentlari va boshqa yuqori-haroratli qismlar kabi samolyot dvigatel qismlarini ishlab chiqarish uchun ishlatiladi; neft sanoatida korroziyaga{2}}bardoshli va yuqori{3}}haroratga chidamli uskunalar, masalan, neft quduqlari korpuslari, klapanlar va quvur liniyasi tizimlarini ishlab chiqarishda foydalanish mumkin; kimyo sanoatida korroziyaga chidamliligini talab qiluvchi uskunalar, masalan, kimyoviy reaktorlar, distillash minoralari, katalizator tashuvchilar va boshqalar ko'pincha undan foydalanadi; yadro sanoatida yadro reaktorlari va yadro yoqilg'isini qayta ishlash uskunalari-korroziyaga chidamli qismlar ham Inconel625 qotishmasidan foydalanadi; va dengiz muhandisligi, tuzsizlantirish zavodi uskunalari, dengizda neft qazib olish uskunalari va dengiz platformasini qo'llab-quvvatlovchi tuzilmalar va dengiz suvi korroziyasiga duchor bo'lgan boshqa qismlardan foydalanish orqali uzoq-muddatli va ishonchli korroziyadan himoyalanish mumkin.Inconel 625 qotishmasi.

 

 2. Kimyoviy tarkibi va mikro tuzilishi xususiyatlari
(I) Kimyoviy elementlarning tarkibi
ning asosiy kimyoviy elementlariInconel 625 qotishmasinikel (Ni), xrom (Cr), molibden (Mo), niobiy (Nb) va boshqalarni o'z ichiga oladi, shuningdek, oz miqdorda temir (Fe), kobalt (Co), titan (Ti), uglerod (C) va boshqa elementlarni o'z ichiga oladi. Quyida har bir elementning qotishmadagi roli keltirilgan
(II) Mikrotuzilma xususiyatlari
Rolik uchunInconel 625 qotishmasi, u odatda ostenit morfologiyasini taqdim etadi, ko'p sonli nozik deformatsiya egizaklari va segregatsiyasi va karbid ikkinchi fazasining mavjudligi. Uning donasi kattaligi (15±2,5)mkm boʻlib, -burchak chegaralari yuqoriroq va dislokatsiya zichligi kattaroq va (111) yoʻnalishda imtiyozli oʻsish kuzatiladi.

2. Chemical composition and microstructure characteristics (I) Chemical element composition The main chemical elements of Inconel625 alloy include nickel (Ni), chromium (Cr), molybdenum (Mo), niobium (Nb), etc., and also contain a small amount of iron (Fe), cobalt (Co), titanium (Ti), carbon (C) and other elements. The following is the role of each element in the alloy (II) Microstructure characteristics For rolled Inconel625 alloy, it presents a typical austenite morphology, with a large number of fine deformation twins and segregation, and the presence of carbide second phase. Its grain size is (15±2.5)μm, with more high-angle grain boundaries and larger dislocation density, and preferential growth in the (111) direction. The Inconel625 alloy prepared by SLM (selective laser melting) has finer cellular crystals inside the molten pool, coarser cellular crystals outside the molten pool, and columnar crystals growing perpendicular to the molten pool boundary. The grain size inside the molten pool is in the range of 0.2-2μm. The SLM-formed alloy has the strongest grain texture characteristics on the XZ plane, the strongest (001) orientation, and its dislocation density is lower than that of the rolled alloy. The grain boundary orientation difference is mainly distributed in the range of 20° - 55°. These different microstructures have an important influence on the properties of the alloy. For example, at 900°C, the oxidation resistance of the rolled Inconel625 alloy is better than that of the SLM alloy. This is mainly attributed to the fact that the rolled alloy has more dislocations and twins. The higher dislocation density is conducive to improving the oxidation resistance of the Inconel625 alloy. Different grain morphology, size and grain boundary characteristics will also affect the strength, hardness, fatigue resistance and other mechanical properties of the alloy to a certain extent, making them suitable for different working conditions and processing requirements.2. Chemical composition and microstructure characteristics (I) Chemical element composition The main chemical elements of Inconel625 alloy include nickel (Ni), chromium (Cr), molybdenum (Mo), niobium (Nb), etc., and also contain a small amount of iron (Fe), cobalt (Co), titanium (Ti), carbon (C) and other elements. The following is the role of each element in the alloy (II) Microstructure characteristics For rolled Inconel625 alloy, it presents a typical austenite morphology, with a large number of fine deformation twins and segregation, and the presence of carbide second phase. Its grain size is (15±2.5)μm, with more high-angle grain boundaries and larger dislocation density, and preferential growth in the (111) direction. The Inconel625 alloy prepared by SLM (selective laser melting) has finer cellular crystals inside the molten pool, coarser cellular crystals outside the molten pool, and columnar crystals growing perpendicular to the molten pool boundary. The grain size inside the molten pool is in the range of 0.2-2μm. The SLM-formed alloy has the strongest grain texture characteristics on the XZ plane, the strongest (001) orientation, and its dislocation density is lower than that of the rolled alloy. The grain boundary orientation difference is mainly distributed in the range of 20° - 55°. These different microstructures have an important influence on the properties of the alloy. For example, at 900°C, the oxidation resistance of the rolled Inconel625 alloy is better than that of the SLM alloy. This is mainly attributed to the fact that the rolled alloy has more dislocations and twins. The higher dislocation density is conducive to improving the oxidation resistance of the Inconel625 alloy. Different grain morphology, size and grain boundary characteristics will also affect the strength, hardness, fatigue resistance and other mechanical properties of the alloy to a certain extent, making them suitable for different working conditions and processing requirements.

SLM (selektiv lazerli eritish) tomonidan tayyorlangan Inconel 625 qotishmasi eritilgan hovuz ichida nozik hujayrali kristallarga, eritilgan hovuz tashqarisida qo'polroq hujayra kristallariga va eritilgan hovuz chegarasiga perpendikulyar o'sadigan ustunli kristallarga ega. Eritilgan hovuz ichidagi don hajmi 0,2-2 mkm oralig'ida. SLM hosil bo'lgan qotishma XZ tekisligida eng kuchli don to'qimalarining xususiyatlariga ega, eng kuchli (001) yo'nalishi va uning dislokatsiya zichligi prokat qotishmasidan pastroqdir. Don chegarasi orientatsiyasi farqi asosan 20 daraja - 55 daraja oralig'ida taqsimlanadi.


Ushbu turli xil mikro tuzilmalar qotishma xususiyatlariga muhim ta'sir ko'rsatadi. Masalan, 900 gradusda haddelenmiş Inconel 625 qotishmasining oksidlanish qarshiligi SLM qotishmasidan yaxshiroqdir. Bu, asosan, prokatlangan qotishma ko'proq dislokatsiya va egizaklarga ega ekanligi bilan bog'liq. Yuqori dislokatsiya zichligi Inconel 625 qotishmasining oksidlanish qarshiligini yaxshilashga yordam beradi. Turli xil don morfologiyasi, hajmi va don chegarasi xususiyatlari, shuningdek, qotishmaning mustahkamligi, qattiqligi, charchoqqa chidamliligi va boshqa mexanik xususiyatlariga ma'lum darajada ta'sir qiladi va ularni turli ish sharoitlari va qayta ishlash talablariga moslashtiradi.

 

 3. Ajoyib ishlash
(I) Korroziyaga chidamlilik
Inconel 625 qotishmasi korroziyaga chidamliligi bo'yicha mukammal ishlashga ega va turli xil korroziy vositalar bilan osonlikcha bardosh bera oladi. Nitrat kislota, xlorid kislota, sulfat kislota va boshqalar kabi kislotali muhitlar va ularning aralash kislotalari bilan qotishma juda past korroziya tezligini ko'rsatadi.
Aynan shu ajoyib korroziyaga chidamliligi tufayli Inconel 625 qotishmasi ko'plab sohalarda keng qo'llaniladi. Kimyo sanoatida ko'pincha reaktorlar, issiqlik almashinuvchilari, nasoslar va klapanlar va boshqalar kabi turli xil korroziv vositalar ostida ishlaydigan asbob-uskunalar va quvurlarni ishlab chiqarish uchun foydalaniladi, bu uskunaning uzoq vaqt davomida barqaror ishlashini ta'minlash va texnik xizmat ko'rsatish va almashtirish chastotasini kamaytirish; dengiz muhandisligi sohasida dengiz suvi korroziyasi bilan tahdid qilingan tuzsizlantirish zavodi uskunalari va dengizda neft ishlab chiqarish uskunalari kabi komponentlar dengiz suvi eroziyasiga samarali qarshilik ko'rsatishi va ishonchli ishlashi mumkin.
(II) Yuqori harorat ko'rsatkichlari
Inconel 625 qotishmasi past haroratdan yuqori haroratli muhitga (masalan, taxminan 980 daraja) yaxshi ishlashga ega.
Shu sababli, Inconel 625 qotishmasi aerokosmik dvigatellar kabi yuqori haroratli sahnalarda, masalan, yuqori haroratli dvigatel qismlari, yonish kameralari, nozullar va boshqalarni ishlab chiqarishda asosiy ilovalarga ega. Bu yuqori harorat va unumdorlik talab qiladigan- qismlarda qotishma aerokosmik uskunalarning normal ishlashini ta'minlash uchun barqaror ishlashi mumkin.
(III) Antioksidlanish samaradorligi
Inconel 625 qotishmasi mukammal antioksidant ko'rsatkichga ega, bu asosan kimyoviy tarkibidagi turli elementlarning sinergik ta'siri bilan bog'liq. Ular orasida xrom yuqori haroratda qotishma yuzasida zich xrom oksidi plyonka hosil qiladi. Ushbu film kislorod kabi oksidlovchi moddalarning kirib borishini samarali ravishda oldini oladi va ichki metallning yanada oksidlanishiga yo'l qo'ymaydi. Nikel qotishmaga yaxshi asosiy oksidlanish qarshiligini beradi, bu esa oksidlovchi muhitda o'zining barqaror ishlashini saqlab qolish imkonini beradi. Shu bilan birga, molibden va niobiy kabi elementlar ham bilvosita qotishmaning oksidlanish qarshiligiga hissa qo'shadi va uning umumiy oksidlanish qarshiligini yaxshilaydi.
(IV) Mexanik xususiyatlar
Inconel 625 qotishmasining kuchlanish kuchi nisbatan yaxshi. Xona haroratida kuchlanish kuchi 830MPa yoki undan yuqori bo'lishi mumkin. Yuqori haroratli muhitda u mos keladigan harorat oralig'ida yuqori kuchlanish darajasini saqlab turishi mumkin, bu esa kuchlanishga duchor bo'lganda sindirish oson emasligini ta'minlaydi. Oqim kuchi jihatidan u odatda 415 MPa dan katta yoki unga teng bo'ladi, ya'ni kuch ma'lum darajaga etgunga qadar barqaror shakl va ishlashni saqlab turishi mumkin va plastik deformatsiyaga osonlikcha duch kelmaydi.

 

 4. Turli xil mahsulot spetsifikatsiyalari va ta'minot holati
Inconel 625 qotishmasi turli xil mahsulot xususiyatlari va ta'minot holatiga ega. Umumiy mahsulot shakllari turli sohalarda mijozlarning turli ehtiyojlarini qondira oladigan choksiz quvurlar, po'lat plitalar, yumaloq po'lat, zarblar, gardishlar, payvandlangan quvurlar, qo'llab-quvvatlovchi payvandlash materiallari va boshqalarni o'z ichiga oladi.