Gnee Steel - ASTM B637 Inconel 718 barlarining etakchi Xitoy yetkazib beruvchisi, ishlab chiqaruvchisi va eksportchisi. UNS N07718 bar nomi bilan ham tanilgan bu nikel qotishma novda mukammal payvandlanish qobiliyatini va payvand chokidan keyingi yorilishlarga- qarshilik ko'rsatadi. Ushbu qotishma 718 barlar, shuningdek, WNR 2.4668 barlar sifatida ham tanilgan, kimyoviy ishlov berish, aerokosmik, suyuq yonilg'i raketa dvigateli komponentlari, ifloslanishni nazorat qilish uskunalari, yadroviy reaktorlar, kriogen saqlash tanklari, klapanlar, mahkamlagichlar, buloqlar, mandrellar, quvur ilgichlari, quduqlarni o'chirish moslamalari {8}B) kabi turli sohalarda keng qo'llaniladi. gaz turbinali dvigatel komponentlari va boshqalar.
So'rov yuborish
Hozir chat

Xitoyning yetakchi yetkazib beruvchi va ishlab chiqaruvchisi sifatida GNEE Steel nikel asosidagi qotishma mahsulotlarni-tejamkorlik bilan ta'minlaydi.

Mahsulotni tanishtirish

 

Inconel 718 Rod tavsifi

 

Gnee SteelXitoyning yetakchi yetkazib beruvchisi, ishlab chiqaruvchisi va eksportchisi hisoblanadiASTM B637 Inconel 718 bar. Bu nikel qotishma bar, shuningdek, deb nomlanuvchiUNS N07718 bar, ajoyib payvandlanish qobiliyati va-payvand chokining qarishi yorilishlariga qarshilik ko‘rsatadi. BularQotishma 718 bar, shuningdek, WNR 2.4668 barlar sifatida ham tanilgan, kimyoviy ishlov berish, aerokosmik, suyuq yonilg'i raketa dvigateli komponentlari, ifloslanishni nazorat qilish uskunalari, yadro reaktorlari, kriogen saqlash tanklari, klapanlar, mahkamlagichlar, buloqlar, mandrellar, quvur ilgichlari, quduq boshini tugatish uskunalari va üfleme dvigatellari (OP) kabi turli sohalarda keng qo'llaniladi. va boshqalar.

 

 

p20241206133619606f8

GNEE Inconel 718 rod

 

Inconel 718 dumaloq novdalar nikel{1}}xrom yuqori-haroratli UNS N07718 qotishmasidan tayyorlangan qattiq silindrsimon novdalar boʻlib, ekstremal muhitlarga bardosh bera oladigan ajoyib mustahkamlik va chidamlilikka ega. Nikel, xrom, molibden, titan, temir, alyuminiy va niobiydan iborat bo'lib, u mukammal korroziyaga chidamlilik va yuqori{5}}harorat ko'rsatkichlarini namoyish etadi, taxminan 1300 daraja (704 daraja) haroratga bardosh beradi. Inconel 718 ham yuqori, ham past haroratlarga chidamli bo'lib, uni turbinalar, reaktiv dvigatellar, boshqaruv rodlari, samolyot korpusi komponentlari va kriogen saqlash tanklari kabi muhim ilovalar uchun javob beradi. Ushbu dumaloq barlar aerokosmik, dengiz, kimyo va harbiy sanoatda viteslar, miller, o'qlar, volanlar va choksiz quvurlarni ishlab chiqarish uchun keng qo'llaniladi. Ular ASTM B637, UNS, ASME, ANSI va EN kabi standartlarga mos keladigan yumaloq, olti burchakli, tekis va kvadrat kabi turli shakllarda mavjud bo'lib, diametri 0,5 mm dan 500 mm gacha va uzunligi 50 mm dan 6000 mm gacha.

 

Gnee Steel kompaniyasida biz har xil oʻlcham va qalinlikdagi yuqori sifatli Inconel 718 Barni{0}} taklif etamiz hamda loyihangizning maxsus ehtiyojlarini qondirish uchun maxsus kesish, sirtni qayta ishlash va global yetkazib berish xizmatlarini taqdim etamiz.

Hozir bog'laning

Inconel 718 Round Bar spetsifikatsiyasi

 

Spetsifikatsiya

ASTM B637 / ASME SB 637

UNS belgisi

N07718

Werkstoff Nr.

2.4668

Boshqa standartlar

AMS 5662, AMS 5663, AMS 5664, SAE AMS 5962, NACE MR0175

Shakllar

Dumaloq, kvadrat, olti burchakli, tekis, zarb qilingan, to'rtburchak, ignabargli

Dumaloq bar o'lchamlari

Diametri 4 mm dan 500 mm gacha

Kvadrat bar o'lchamlari

18 mm dan 47 mm gacha

Olti burchakli bar o'lchamlari

18 mm dan 57 mm gacha

Yassi bar o'lchamlari

12,7 mm dan 254 mm gacha kengligi, 2 mm dan 150 mm gacha qalinligi

Uzunlik

1 dan 6 metrgacha, Maxsus kesish uzunligi

Tugatish

Qora, Yorqin sayqallangan, qo'pol burilishli, №4 pardozlash, Mat Finish, BA Finish

Vaziyat

Issiq haddelenmiş, sovuq tortilgan, tavlangan, yog'ingarchilik bilan qattiqlashtirilgan, zarb qilingan

 

Inconel 718 BarSpetsifikatsiya

 

Inconel 718 dumaloq barlarning ekvivalent darajasi

Standart Werkstoff Nr. UNS AFNOR
Inconel 718 2.4668 N07718 NC19FeNb

 

Inconel 718 dumaloq barning kimyoviy tarkibi

Baho Mn Ni S Cr Mo Cu Si C Co
Inconel 718 0,035 maksimal 50 – 55 0,015 maksimal 17 – 21 2.8 – 3.3 0,3 maksimal 0,035 maksimal 0,08 maksimal 1,0 maks

 

AMS 5664 Inconel 718 Hex Bar mexanik xususiyatlari

Zichlik Uzaytiruvchi Hosildorlik xususiyatlari Erish nuqtasi Kuchlanish xususiyatlari
8,02 g/sm3 45 % Psi – 70 000 , MPa – 482 (2460 daraja F) 1350 daraja Psi – 135 000 , MPa – 930

 

Inconel 718 quvurlarni o'rnatish texnik ma'lumotlar varag'i

 

Inconel 718 dumaloq barning o'lchamlari va o'lchamlari
Metrik AQSh bari ASTM / Kanada yapon
Bar hajmi Diam. (mm) Bar hajmi Diam. (dyuym) Bar hajmi Diam. (mm2) Bar hajmi Diam. (mm)
5 5 #2 0.250 10M 100 6 6
5.5 5.5 #3 0.375 15M 200 10 10
6 6 #4 0.500 20M 300 13 13
7 7 #5 0.718 25M 500 16 16
8 8 #6 0.750 30M 700 19 19
9 9 #7 0.875 35M 1000 22 22
10 10 #8 1.000 45M 1500 25 25
11 11 #9 1.125 55M 2500 29 29
12 12 #10 1.250     32 32
14 14 #11 1.375     35 35
16 16 #12 1.500     38 38
18 18 #13 1.718     41 41
20 20 #14 1.750     44 44
22 22 #15 1.875     48 48
25 25 #16 2.000     51 51
28 28 #18 2.250     57 57
32 32            
36 36            
40 40            
44 44            
50 50            

 

Inconel 718 dumaloq novda vazni jadvali

Dumaloq bar
Hajmi Kg / fut Kg / Mtr Hajmi Kg / fut Kg / Mtr Hajmi Kg / fut Kg / Mtr
3 mm 0.017 0.055 20 mm 0.753 2.470 3" 10.900 35.762
1/8" 0.019 0.062 22 mm 0.908 2.979 3-1/4" 12.800 41.996
5/32" 0.029 0.095 7/8" 0.926 3.038 3-1/2" 14.850 48.772
4 mm 0.030 0.098 24 mm 1.080 3.543 3-3/4" 17.001 55.780
3/16" 0.043 0.141 25 mm 1.180 3.871 4" 19.306 63.340
5 mm 0.047 0.154 1" 1.210 3.970 4-1/4" 21.908 72.249
7/32" 0.058 0.190 26 mm 1.271 4.170 4-1/2" 24.4487 80.340
6 mm 0.068 0.223 27 mm 1.368 4.490 4-3/4" 27.366 90.249
1/4" 0.076 0.249 1-1/8" 1.534 5.033 5" 30.461 99.940
7 mm 0.091 0.298 30 mm 1.691 5.548 5-1/2" 36.690 121.000
5/16" 0.118 0.387 1-1/4" 1.924 6.349 6" 43.860 143.900
8 mm 0.120 0.398 32 mm 1.894 6.314 6-1/2" 51.093 167.630
9 mm 0.152 0.498 1-3/8" 2.303 7.550 7" 59.432 196.000
3/8" 0.170 0.557 35 mm 2.390 7.553 7-1/2" 68.226 225.000
10 mm 0.189 0.620 36 mm 2.438 7.999 8" 77.586 254.55
11 mm 0.228 0.748 38 mm 2.792 8.903 10" 121.048 397.140

 

Inconel 718 dumaloq bar ishlab chiqarish jarayoni

 

Inconel 718 Round Bar Manufacturing Process

Inconel 718 dumaloq bar ishlab chiqarish jarayoni

 

Inconel 718 Bar zaxirada mavjud va shoshilinch ehtiyojlarni qondirish uchun darhol jo'natilishi mumkin.

 

UNS N07718 Bright Bar

UNS N07718 Yorqin bar

DIN 2.4668 Hex Bar

DIN 2.4668 Hex Bar

Inconel Alloy 718 Square Bar

Inconel qotishmasi 718 kvadrat bar

Werkstoff 2.4668 Rectangular Bar

Werkstoff 2.4668 To'rtburchaklar bar

Nickel 718 Hexagonal Bar

Nikel 718 olti burchakli bar

Nickel Alloy 718 Black Bar

Nikel qotishmasi 718 qora bar

Inconel 718 Cold Drawn Bar

Inconel 718 sovuq chizilgan bar

Inconel Alloy 718 Flat Bar

Inconel Alloy 718 Flat Bar

AMS 5664 Hot Rolled Bar

AMS 5664 Issiq haddelenmiş bar

 

Gnee Steel tomonidan taqdim etilgan mahsulotlar va xizmatlar

 

Inconel 718 Bar ilovalari

 

Aerokosmik: reaktiv dvigatel komponentlari, gaz turbinasi qismlari, raketa dvigatellari va mahkamlagichlar.

Neft va gaz: Quduq burg'ilash quvurlari, quduq boshi qismlari, klapanlar va nasos agregatlari.

Kimyo sanoati: yuqori haroratli reaktorlar va quvurlar.-

Dengiz: suv osti kemalari komponentlari va yuqori-kuchli vallar.

Yadro energetikasi: reaktor yadrosi va boshqaruv rod komponentlari.

Applications of inconel 718 Pipe Fitting

Packaging method for Alloy 718 Pipe Fitting

Qotishma 718 Bar uchun qadoqlash usuli

 

Gnee Steel barcha turdagi yuklarni tashish uchun eng xavfsiz va samarali qadoqlash usullaridan foydalanadi. Bizning qadoqlash usullarimiz quyidagilarni o'z ichiga oladi:

Yog'och qutilar
Yog'och palletlar
Shrink o'ramli qadoqlash
Karton qutilar
Yog'och qutilar (taxta)

 

718 dumaloq bar narxlari ro'yxati

 


Hajmi AQSh dollarida narx
OD1,4 x 11 Uzunlik 130,19 AQSH dollari
Diametri 40 mm x 1,00 Mtr uzunligi 510,02 AQSH dollari
80MM x Uzunlik: 2 Mtr 4 044,51 AQSH dollari
Diametri 60 MM x 1,00 Mtr uzunligi 1186,65 AQSH dollari
Diametri 100 MM x 0,50 Mtr uzunligi 1661,67 AQSH dollari
88 MM Dia x 600 mm Lg 15,68 AQSH dollari

 

Gnee Steel haqida

 

Inconel 718 Round Bar

 

Gnee Steel haqida

Eng oxirgisini so'ranginconel 718 barnarxlar ro'yxati. Iltimos, qo'ng'iroq qiling+8615824687445yoki elektron pochtass@gneesteel.commavjud zaxiralar va so'nggi narxlar ro'yxati haqida ma'lumot olish uchuninconel 718 bar.

modular-1
Sizga kerak bo'lgan Inconel 718 Bar uchun tezkor taklifni olish uchun biz bilan bog'laning

Gnee Steel 718 Inconel ANSI B16.11 quvur armatura, ASTM B{2}} tishli armatura, Inconel qotishma 718 ASME SB 564 Class 3000 zarb qilingan tishli armatura, 718 qotishma sinfi 206/Class quvur fittinglari Xitoyning yetakchi ishlab chiqaruvchilari va yetkazib beruvchilaridan biridir. 6000 ta zarb qilingan rozetkali payvandlash quvurlari armaturalari, ASTM B564 718 ANSI 3000 lb muftalar va ASME SB 564 718 9000 toifali quvur armaturalari ularni eng raqobatbardosh narxlarda yetkazib beradi.

TSS

Savol: Inconel 718 qanday maqsadlarda ishlatiladi?

Javob: Inconel 718 juda yuqori quvvat, korroziyaga chidamlilik va yuqori{1}}haroratga chidamlilik talab qiladigan sohalarda qo‘llaniladi. Odatda aerokosmik komponentlar, gaz turbinalari, bosimli idishlar va kimyoviy uskunalarda qo'llaniladi. Uning ekstremal muhitda mukammal ishlashini saqlab turish qobiliyati uni yuqori{4}}harorat va yuqori{5}}bosimli ilovalar uchun ideal tanlov qiladi.

Savol: Inconel 718 dumaloq barlarning asosiy ilovalari qanday?

Javob: Odatda aerokosmik, kimyo, energiya ishlab chiqarish va dengiz sanoatida turbinali pichoqlar, klapanlar va bosimli idishlar kabi komponentlar uchun ishlatiladi.

Issiq teglar: inconel 718 rod, Xitoy inconel 718 rod yetkazib beruvchilari

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov