Incoloy 800 Flat Face Flange
video

Incoloy 800 Flat Face Flange

Incoloy 800 Flange Quick Info

NPS: 1/2 - 48"
Pressure Rating: 150 - 2500 lbs
Sizes: Sch 5 - XXS
So'rov yuborish
Hozir chat

Xitoyning yetakchi yetkazib beruvchi va ishlab chiqaruvchisi sifatida GNEE Steel nikel asosidagi qotishma mahsulotlarni-tejamkorlik bilan ta'minlaydi.

Mahsulotni tanishtirish

 

Incoloy 800 Flange description

Incoloy 800 Flange
Gnee Steel Incoloy 800 Flange introduce

Incoloy 800 Flanges are furnished with nickel-chromium-iron alloys that intend outstanding resistance and strength at harsh environments. The flanges exhibit superior resistance to chloride stress corrosion cracking and crevice corrosion. Even more, it also shows superior intergranular corrosion, stress rupture and creepy aspects. The welding of these flanges is done using various techniques such as MIG, TIG and more.

Incoloy 800 Flange ASME B16.5 We are renowned in the industry for producing various types of high-quality flanges to meet the needs of our clients. We produce reliable and high-quality incoloy 800 flanges. We use premium resources and advanced machinery to produce ASTM B564 UNS N08800 Incoloy 800 Flanges.

dimensions-of-incoloy-800-flanges

RF Dia. (R) No. of Bolt Holes Min. Thickness (T) Dia. of Hub Top (HT) Dia. Hub Base (HB)
1⁄2 3.50 1.38 0.62 4 0.38 2.38 0.62 0.88 0.84 1.19 1.81 0.56
3⁄4 3.88 1.69 0.62 4 0.44 2.75 0.82 1.09 1.05 1.50 2.00 0.56
1 4.25 2.00 0.62 4 0.50 3.12 1.05 1.36 1.32 1.94 2.12 0.62
11⁄4 4.62 2.50 0.62 4 0.56 3.50 1.38 1.70 1.66 2.31 2.19 0.75
11⁄2 5.00 2.88 0.62 4 0.62 3.88 1.61 1.95 1.90 2.56 2.38 0.81
2 6.00 3.62 0.75 4 0.69 4.75 2.07 2.44 2.38 3.06 2.44 0.94
21⁄2 7.00 4.12 0.75 4 0.81 5.50 2.47 2.94 2.88 3.56 2.69 1.06
3 7.50 5.00 0.75 4 0.88 6.00 3.07 3.57 3.50 4.25 2.69 1.12
31⁄2 8.50 5.50 0.75 8 0.88 7.00 3.55 4.07 4.00 4.81 2.75 1.19
4 9.00 6.19 0.75 8 0.88 7.50 4.03 4.57 4.50 5.31 2.94 1.25
5 10.00 7.31 0.88 8 0.88 8.50 5.05 5.66 5.56 6.44 3.44 1.38
6 11.00 8.50 0.88 8 0.94 9.50 6.07 6.72 6.63 7.56 3.44 1.50

Incoloy 800 Flat Face Flange Specification

Chemical Equation of Nickel Alloy 800 Flange

C S
800 0.10 max 1.50 max 1.00 max 0.015 max 0.75 max 39.50 min 30.00 – 35.00 19.00 – 23.00 0.15 – 0.60 0.15 – 0.60

Nickel Alloy 800 Flange Pressure Rating

Temp., ℃ Incoloy 800 Flanges Working Pressures by Classes, bar
  150 300 400 600 900 1500 2500
-29 ~ 38 20.0 51.7 68.9 103.4 155.1 258.6 430.9
50 19.5 51.7 68.9 103.4 155.1 258.6 430.9
100 17.7 51.5 68.7 103.0 154.6 257.6 429.4
150 15.8 50.3 66.8 100.3 150.6 250.8 418.2
200 13.8 48.6 64.8 97.2 145.8 243.4 405.4
250 12.1 46.30 61.7 92.7 139.0 231.8 386.2
300 10.2 42.9 57.0 85.7 128.6 214.4 357.1
325 9.3 41.4 55.0 82.6 124.0 206.6 344.3
350 8.4 40.3 53.6 80.4 120.7 201.1 335.3
375 7.4 38.9 51.6 77.6 116.5 194.1 323.2
400 6.5 36.5 48.9 73.3 109.8 183.1 304.9
425 5.5 35.2 46.5 70.0 105.1 175.1 291.6
450 4.6 33.7 45.1 67.7 101.4 169.0 281.8
475 3.7 31.7 42.3 63.4 95.1 158.2 263.9
500 2.8 28.2 37.6 56.5 84.7 140.9 235.0
538 1.4 16.5 22.1 33.1 49.6 82.7 137.9
550 - 13.9 18.6 27.9 41.8 69.7 116.2
575 - 9.4 12.6 18.9 28.3 47.2 78.6
600 - 6.6 8.9 13.3 19.9 33.2 55.3
625 - 5.1 6.8 10.3 15.4 25.7 42.8
650 - 4.7 6.3 9.5 14.2 23.6 39.4

UNS N08800 Flanges Flange Faces

UNS N08800 Flanges Flange Faces

Face Type of Incoloy 800 Flanges
A
F
G
D
E
H O-Ring Groove
B
C

Incoloy 800 Flat Face Flange packing

Gnee Steel Incoloy 800 Flat Face Flange packing

Gnee Steel Incoloy 800 Flat Face Flange packing
Gnee Steel Incoloy 800 Flat Face Flange packing

Issiq teglar: Incoloy 800 Flat Face Flange, China Incoloy 800 Flat Face Flange suppliers

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov